| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Antimony (Sb) <100>•0.005–0.02 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Antimony-doped to a verified resistivity of 0.005–0.02 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Heavily Antimony (Sb)-doped to 0.005–0.02 Ω·cm (N+) (~1.5×1018–1.2×1019 cm-3 donor concentration), Antimony exhibits very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion (“autodoping”) during elevated-temperature LPCVD and epitaxial processes. It serves as an industry-standard low-resistance 200 mm base for abrupt silicon epitaxy, trench power MOSFETs, discrete Schottky barriers, and buried-layer R&D.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Antimony (Sb) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.005–0.02 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
- 200 mm CMOS, MEMS & Power Semiconductor Prototyping: Cleanroom <100> crystal plane supports KOH/TMAH anisotropic etching, Bosch DRIE, epitaxial growth, and pilot-line CMOS process integration;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Antimony-doped (0.005–0.02 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type Antimony (100), 0.005-0.02 ohm-cm, 725 um, SSP (This Product) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type (0.005–0.02 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade 200 mm antimony-doped silicon wafers require cleanroom handling to preserve CMP surface quality and prevent particulate contamination. Storage must occur in dry nitrogen or desiccator environments to minimize native oxide growth and organic contamination.
- Cleanroom Environment Requirement: All handling must occur in a cleanroom environment using vacuum wands or PTFE/PEEK tweezers applied only to the wafer perimeter edge.
- Storage Atmosphere Control: Store wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Native Oxide Sensitivity: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, requiring controlled atmosphere storage to minimize uncontrolled oxidation before processing.
- Surface Contamination Prevention: Avoid all direct surface contact during handling and storage to maintain the Ra < 0.5 nm CMP finish and prevent particle contamination exceeding ≤ 10 particles per wafer.
- Wet Processing Safety Requirement: All wet-chemical processing including RCA clean and native oxide removal must be performed in an exhaust fume hood or automated wet bench following institutional EHS and SDS protocols.
This protocol describes the sequential steps for safe handling, pre-cleaning, and surface preparation of prime-grade 200 mm antimony-doped silicon wafers. Each step preserves the CMP surface quality and prevents contamination during cleanroom processing.
Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or automated wet bench
- Inspect Cassette and Wafer Condition
Inspect the cleanroom cassette and wafer edges for visible particulate contamination or damage before removing any wafer. - Transfer Wafer Using Cleanroom Tools
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge. - Perform Solvent Pre-Cleaning Sequence
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water followed by nitrogen blow-drying. - Apply Plasma Descum Treatment
Apply a mild oxygen plasma descum to the wafer surface prior to photoresist spin coating or PVD/ALD deposition. - Remove Native Oxide in Controlled Environment
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench using facility-approved protocols. - Store Unused Wafers in Controlled Atmosphere
Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator.
Why is antimony used as the N-type dopant in this 8-inch silicon wafer instead of phosphorus or arsenic?
Antimony (Sb) is selected for its very low solid-state diffusivity and exceptionally low vapor-phase out-diffusion, which suppresses autodoping during elevated-temperature LPCVD and epitaxial processes. This wafer is doped to 0.005–0.02 Ω·cm (N+), corresponding to roughly 1.5×10^18–1.2×10^19 cm^-3 donor concentration, making it an industry-standard low-resistance 200 mm base for abrupt silicon epitaxy, trench power MOSFETs, and discrete Schottky barriers. The trade-off versus arsenic or phosphorus is a narrower achievable resistivity window, but with superior dopant profile stability at high thermal budgets.
Can this 200 mm antimony-doped wafer be used directly in automated FOUP-based cluster tools and stepper lithography without additional edge preparation?
Yes. The wafer meets SEMI M1 200 mm standards with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a single SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90° angle), ensuring reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools. The SSP front surface has Ra < 0.5 nm, TTV < 5 μm, and bow/warp < 30 μm, which supports uniform nucleation for epitaxy, PVD/CVD, ALD, and scanner lithography. No secondary flat or notch is present, consistent with the standard 200 mm single-notch configuration.
What storage and handling conditions are required to maintain the surface quality of this prime-grade antimony-doped silicon wafer before processing?
Wafers must be stored sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors to preserve the CMP mirror finish (Ra < 0.5 nm) and prevent organic contamination. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers; never contact the polished face. The supplied 200 mm cleanroom protective cassettes (5, 10, or 25 pcs) immobilize wafer edges during transit, but unused wafers should remain in the original cassette or a FOUP carrier under dry nitrogen.
This 200 mm prime CZ N-type antimony-doped silicon wafer combines a low-diffusivity N+ substrate (0.005–0.02 Ω·cm) with SEMI M1 notch geometry and sub-nanometer CMP finish, making it well-suited for abrupt epitaxy, power MOSFET prototyping, and automated 200 mm tool lines. Its bare SSP surface and tight TTV/bow tolerances demand disciplined cleanroom handling and pre-clean protocols to preserve interface quality.
Positive
- Low-diffusivity antimony N+ substrate: Antimony doping at 0.005–0.02 Ω·cm exhibits very low solid-state diffusivity and minimal vapor-phase autodoping, supporting abrupt epitaxial interfaces and buried-layer structures during high-temperature LPCVD and epi steps.
- SEMI M1 200 mm tool compatibility: Standardized 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and SEMI V-notch along <110> enable reliable alignment and transport across FOUP cassettes, cluster tools, steppers, CMP polishers, and RTP chambers.
Trade-offs
- Bare surface requires pre-clean: Uncoated prime silicon forms a ~1–2 nm native SiO2 layer in ambient air, so native-oxide removal or RCA clean must precede metallization or epitaxy, requiring wet-bench infrastructure and EHS-compliant protocols.
- Strict cleanroom storage required: Sub-nanometer CMP finish and ≤10 particles/wafer specification demand sealed cassette or FOUP storage in dry nitrogen cabinets away from particulates and corrosive vapors to preserve surface quality.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).