| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Arsenic (As) <111>•0.001–0.005 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Arsenic-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Degenerately Arsenic (As)-doped to 0.001–0.005 Ω·cm (N++) (~1019–7×1019 cm-3 donor density), Arsenic matches the covalent atomic radius of silicon closely to minimize lattice strain and misfit dislocations at ultra-high doping while diffusing roughly an order of magnitude slower than Phosphorus. This makes heavily As-doped 200 mm wafers the benchmark substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-resistance vertical ohmic contacts.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Arsenic (As) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
- Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Arsenic-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type Arsenic (111), 0.001-0.005 ohm-cm, 725 um, SSP (This Product) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade arsenic-doped silicon substrates require particulate-controlled storage and edge-only contact to preserve CMP surface quality. Ambient native oxide growth and moisture exposure must be managed prior to epitaxy or metallization.
- Cleanroom Storage Atmosphere: Store wafers sealed in the original polypropylene cassette or FOUP within a dry nitrogen cabinet or cleanroom desiccator to limit airborne organic contamination and native oxide growth.
- Surface Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent scratching or contaminating the mirror-polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, which must be removed via RCA clean or wet processing before epitaxy or ohmic contact formation.
- Wet Processing Containment: Perform all wet-chemical cleaning and etching inside an exhaust fume hood or automated wet bench under facility-approved EHS and SDS protocols.
- Particulate and Vapor Exposure: Avoid exposure to particulate dust and corrosive vapors during storage and transfer to maintain the ≤10 particles per wafer specification.
This procedure covers safe removal from packaging, pre-cleaning, and preparation of prime 200 mm silicon wafers for thin-film deposition or lithography. Steps emphasize edge-only contact and contamination control.
Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, 200 mm FOUP or polypropylene cassette, Dry nitrogen cabinet or desiccator
- Inspect Packaging Integrity
Verify the cleanroom cassette seal is intact and check for visible particulate contamination before opening. - Transfer Wafer by Edge
Remove the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Perform Solvent Pre-Cleaning
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and deionized water, then blow-dry with nitrogen. - Remove Native Oxide
Perform RCA standard clean or buffered oxide etch inside an exhaust fume hood to remove the ambient 1–2 nm native SiO2 layer. - Dry and Load for Processing
Blow-dry the wafer with filtered nitrogen and immediately load it into the deposition or lithography tool to minimize re-oxidation.
Why choose arsenic-doped <111> silicon wafers over phosphorus-doped <100> for 200 mm epitaxy?
Arsenic doping at 0.001–0.005 Ω·cm (N++) provides roughly an order of magnitude slower diffusion than phosphorus, which suppresses dopant out-diffusion and autodoping during high-temperature Si/SiGe epitaxy. The <111> orientation offers a densely packed three-fold surface symmetry with higher in-plane elastic modulus and slower wet alkaline etch kinetics than <100>, making it preferable for GaN-on-Si and III-nitride epitaxy. Additionally, arsenic's covalent atomic radius closely matches silicon, minimizing lattice strain and misfit dislocations at ultra-high doping levels.
Can these 8-inch arsenic-doped wafers be used directly in automated 200 mm FOUP cluster tools?
Yes. The wafers meet SEMI M1 specifications with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°), ensuring compatibility with automated FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The high flexural stiffness of the 725 μm thickness supports reliable robotic handling. The SSP finish with Ra < 0.5 nm and TTV < 5 μm further ensures uniform nucleation for epitaxy and lithography.
What cleanroom storage and handling procedures are required to maintain the surface quality of these prime silicon wafers?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers. For pre-cleaning, degrease sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. Keep unused wafers in the original cleanroom polypropylene cassette or FOUP carrier to minimize airborne organic contamination.
This 200 mm prime CZ silicon wafer combines degenerate Arsenic doping (0.001–0.005 Ω·cm) with a <111> orientation and SSP finish (Ra < 0.5 nm), making it a strong substrate choice for Si/SiGe epitaxy, GaN-on-Si heteroepitaxy, and low-resistance vertical ohmic contact development. Its SEMI M1 geometry and 725 μm thickness support automated 200 mm FOUP and cluster-tool handling, though the bare, uncoated surface and <111> orientation impose specific pre-clean and process-window requirements.
Positive
- Low-Strain Arsenic Doping for Epi: Arsenic's covalent radius closely matches silicon, minimizing lattice strain and misfit dislocations at ultra-high doping, while its roughly order-of-magnitude slower diffusion versus phosphorus preserves abrupt doping profiles during subsequent thermal steps. This makes the substrate well-suited for Si/SiGe epitaxy and low-resistance vertical ohmic contacts.
- SEMI M1 Geometry for Automated Tools: The 200.0 ± 0.2 mm diameter, SEMI V-notch along <110> ± 1°, and 725 ± 25 μm thickness conform to SEMI M1, enabling reliable optical alignment and robotic handling across FOUP cassettes, cluster tools, steppers, CMP polishers, and RTP chambers.
Trade-offs
- Bare Surface Requires Pre-Clean: The wafer is supplied bare with only a native ~1–2 nm SiO2 film; reproducible epitaxy, metallization, or ALD nucleation requires solvent/SC-1 cleaning, N2 dry, and optional O2 plasma descum or RCA clean under institutional EHS protocols before processing.
- <111> Orientation Narrows Process Window: The <111> plane exhibits slower wet alkaline etch kinetics and different surface chemistry than <100> silicon, so etch recipes, cleaning steps, and some lithographic or oxidation processes must be re-qualified rather than transferred directly from <100> baselines.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).