| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Arsenic (As) <100>•0.001–0.005 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Arsenic-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Degenerately Arsenic (As)-doped to 0.001–0.005 Ω·cm (N++) (~1019–7×1019 cm-3 donor density), Arsenic matches the covalent atomic radius of silicon closely to minimize lattice strain and misfit dislocations at ultra-high doping while diffusing roughly an order of magnitude slower than Phosphorus. This makes heavily As-doped 200 mm wafers the benchmark substrate for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-resistance vertical ohmic contacts.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Arsenic (As) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
- 200 mm CMOS, MEMS & Power Semiconductor Prototyping: Cleanroom <100> crystal plane supports KOH/TMAH anisotropic etching, Bosch DRIE, epitaxial growth, and pilot-line CMOS process integration;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Arsenic-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type Arsenic (100), 0.001-0.005 ohm-cm, 725 um, SSP (This Product) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch P-Type <111> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <111> | Hexagonal <111> 200 mm lattice for III-nitride heteroepitaxy |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade arsenic-doped silicon wafers require controlled storage to prevent surface contamination and native oxide growth. Handling must avoid edge chipping and particulate deposition that compromise downstream lithography and epitaxy.
- Atmospheric Storage Requirements: Store wafers sealed in a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and uncontrolled native oxide growth.
- Particulate and Vapor Exposure Limits: Keep wafers away from particulate dust and corrosive vapors that degrade the mirror-polished CMP surface and introduce defect sites.
- Mechanical Handling Constraints: Handle wafers strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface scratches and edge chipping.
- Native Oxide Interface Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxy to ensure reproducible ohmic interfaces.
- Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within exhaust fume hoods or automated wet benches.
Proper handling and pre-cleaning of prime-grade arsenic-doped silicon wafers preserves CMP surface quality and ensures reproducible thin-film interfaces. Sequential solvent cleaning, native oxide control, and controlled storage are required before lithography or deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, 200 mm cleanroom protective cassette or FOUP carrier, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or automated wet bench
- Inspect Cassette and Wafer Edges
Inspect the cleanroom cassette and wafer edges for particulate contamination or mechanical damage before removing wafers. - Transfer Wafers by Perimeter Edge
Transfer wafers strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers to avoid surface contact. - Degrease in Sequential Solvent Baths
Degrease wafers sequentially in electronic-grade acetone, isopropanol, and DI water or perform megasonic/SC-1 cleaning. - Dry with Nitrogen and Plasma Descum
Dry wafers with N2 blow-drying followed by mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove Native Oxide Before Metallization
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench using facility-approved protocols before metallization or epitaxy. - Store Unused Wafers in Nitrogen Cabinet
Store unused wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet.
Why choose arsenic-doped N-type silicon wafers over phosphorus-doped for 200 mm power device fabrication?
Arsenic doping is preferred for ultra-low resistivity N++ substrates because its covalent atomic radius closely matches silicon, minimizing lattice strain and misfit dislocations at high doping levels. Additionally, arsenic diffuses roughly an order of magnitude slower than phosphorus, which preserves abrupt doping profiles during subsequent high-temperature processing steps such as epitaxy or thermal oxidation. This makes arsenic-doped 200 mm wafers ideal for Si/SiGe epitaxy, power MOSFETs, IGBTs, and low-resistance vertical ohmic contacts.
Can these 8-inch arsenic-doped wafers be used directly in automated 200 mm FOUP-compatible tools without additional edge profiling?
Yes. These wafers are manufactured to SEMI M1 standards with a 200.0 ± 0.2 mm diameter, a SEMI V-notch along <110> ± 1°, and a standard 725 ± 25 μm thickness. The mechanical thickness provides high flexural stiffness and is compatible with automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. The precision notch ensures reliable optical alignment across automated handlers and steppers.
What are the recommended storage and handling procedures to maintain the surface quality of these prime-grade silicon wafers?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contamination. The wafers are shipped in 200 mm cleanroom protective cassettes (available in 5, 10, or 25 pcs) that immobilize wafer edges and prevent surface contact during transit.
This 200 mm prime CZ silicon wafer combines degenerate arsenic doping (0.001–0.005 Ω·cm) with a <100> ± 0.5° orientation and SSP finish (Ra < 0.5 nm), making it a strong substrate choice for Si/SiGe epitaxy, power MOSFET/IGBT prototyping, and low-resistance vertical ohmic contacts. Its SEMI M1 geometry and 725 ± 25 μm thickness ensure compatibility with automated 200 mm FOUP, lithography, CMP, and RTP tooling, though successful use requires cleanroom handling and wet-bench infrastructure for native-oxide removal.
Positive
- Arsenic Doping Minimizes Lattice Strain: Arsenic's covalent atomic radius closely matches silicon, reducing misfit dislocations at ultra-high doping, while its roughly order-of-magnitude slower diffusion versus phosphorus preserves abrupt doping profiles during subsequent thermal processing.
- SEMI M1 Geometry for Automated 200 mm Tools: The 200.0 ± 0.2 mm diameter, SEMI V-notch along <110> ± 1°, and 725 ± 25 μm thickness conform to SEMI M1, enabling reliable robotic handling in FOUP cassettes, cluster tools, steppers, CMP polishers, and RTP chambers.
Trade-offs
- Native Oxide Requires Wet-Bench Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; removing it before metallization or epitaxy demands wet processing inside an exhaust fume hood or automated wet bench using facility-approved protocols.
- Cleanroom Handling and Storage Mandatory: To preserve the Ra < 0.5 nm CMP surface and ≤10 particles/wafer specification, wafers must be handled by perimeter edge or robotic end-effectors and stored sealed in a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).