8-Inch N-Type Silicon Wafer 0.001-0.005 Ω·cm ATOMFAIR®

Price range: $299.00 through $1,199.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ 200mm N-type silicon wafer, 725μm, 0.001–0.005 Ω·cm, SSP Ra<0.5nm. SEMI M1 V-notch. In stock.

Diameter & Notch:
8-Inch (200.0 ± 0.2 mm)
SEMI V-Notch <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•0.001–0.005 Ω·cm
Thickness:
725 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current 200 mm device testing.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting 200 mm GaN-on-Si / III-nitride epitaxy, UHV surface studies, and discrete power/bipolar R&D.

8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 8-Inch Notch & Precision

Standardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.

  • Diameter: 200.0 ± 0.2 mm (8.0 Inch)
  • Primary Fiducial: SEMI V-Notch along <110> ± 1° (Depth 1.0 +0.25/-0.00 mm, 90°)
  • Secondary Fiducial: None (SEMI M1 200 mm notch standard)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 200.0 ± 0.2 mm (8-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 725 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Fiducial (Notch) SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) SEMI M1 (200 mm)
Secondary Flat / Notch None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) SEMI M1 / Lot Laser ID
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes 200 mm Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
  • Large-Area GaN/AlN Epitaxy & Power Devices: Dense three-fold <111> crystal lattice supports 200 mm GaN-on-Si/AlN/SiC heteroepitaxy, 2D template growth, and discrete power/bipolar R&D;
  • 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
  • In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 8-Inch (200 mm), N-Type (111), 0.001-0.005 ohm-cm, 725 um, SSP (This Product) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type (0.001–0.005 Ω·cm) SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, P-Type <100> Standard SEMI M1 200 mm notch CMOS & lithography substrate
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) 8-Inch (200 mm) / DSP 725 ± 25 μm, P-Type <100> Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics
8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type <100> Phosphorus-doped 200 mm wafer for power & CMOS R&D
8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped 200 mm epi substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade monocrystalline silicon substrates require particulate-controlled storage and edge-only contact to preserve the CMP mirror finish. Ambient native oxide growth and airborne organic contamination must be managed prior to any thin-film or lithography process.

  • Particulate and Vapor Isolation: Store wafers sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Contact Restriction: Handle wafers strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the polished front surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA standard clean or wet processing before metallization or epitaxy.
  • Wet-Chemical EHS Compliance: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols inside an exhaust fume hood or automated wet bench.

Proper pre-cleaning and native oxide control are required to preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Each step must be performed under cleanroom conditions with edge-only wafer contact.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, 200 mm cleanroom cassette or FOUP carrier, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or automated wet bench

  1. Inspect Cassette Seal
    Verify the cleanroom cassette seal is intact and confirm the wafer lot matches the accompanying Certificate of Analysis before opening.
  2. Transfer by Edge Contact
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease Sequentially
    Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water, or perform a megasonic SC-1 clean.
  4. Dry and Descum
    Blow-dry the wafer with nitrogen and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove Native Oxide
    Perform RCA standard clean or wet oxide removal inside an exhaust fume hood or automated wet bench when metallization or epitaxy requires an oxide-free interface.
  6. Return to Nitrogen Storage
    Return unused wafers to the original cleanroom cassette and store sealed within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a <111> N++ phosphorus-doped 200 mm silicon wafer instead of a standard <100> substrate for GaN epitaxy?

The <111> orientation provides a densely packed three-fold surface symmetry that supports hexagonal GaN/AlN heteroepitaxy, while the degenerately phosphorus-doped bulk (0.001–0.005 Ω·cm, ~10^19–10^20 cm^-3) enables low-resistance backside ohmic contacts and conductive bottom gates. Compared with <100> silicon, the <111> plane also exhibits a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics, which can be advantageous for discrete power and bipolar R&D. Note that this wafer is SSP with a fine-ground back, so double-side-polished bonding or IR-optics applications would require a different finish.

Can this 725 µm SSP 200 mm wafer be used directly in automated FOUP cassettes and cluster tools without additional edge preparation?

Yes. The wafer meets SEMI M1 200 mm geometry with a 200.0 ± 0.2 mm diameter, 725 ± 25 µm thickness, and a single SEMI V-notch along <110> ± 1° (1.0 mm depth, 90°), which is the standard fiducial for automated FOUP handlers, steppers, and cluster tools. Flatness is controlled to TTV < 5 µm and bow/warp < 30 µm, supporting robotic handling and lithographic alignment. The front surface is CMP-polished to Ra < 0.5 nm with ≤ 10 particles per wafer, but the back is fine-ground, so backside particle-sensitive processes may require an additional clean.

What surface preparation is required before epitaxy or metallization on this bare prime silicon wafer?

Bare prime silicon forms a native SiO2 layer of approximately 1–2 nm in ambient air, so native oxide removal or an RCA standard clean is typically required before epitaxy or ohmic metallization. Recommended pre-clean includes sequential electronic-grade acetone, isopropanol, and DI water (or megasonic/SC-1), followed by N2 blow-drying and a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. All wet-chemical processing must be performed in an exhaust fume hood or automated wet bench following institutional EHS and SDS protocols; store unused wafers sealed in the original cleanroom cassette inside a dry nitrogen cabinet.

The 8-inch N-type <111> prime silicon wafer with 0.001–0.005 Ω·cm resistivity and SSP finish provides a low-resistance, crystallographically oriented substrate suited for GaN-on-Si epitaxy and backside ohmic contact formation, while its SEMI M1 geometry ensures compatibility with automated 200 mm tooling. However, its high doping level and <111> orientation impose constraints on thermal budget and etch processing that must be managed through dedicated cleanroom protocols.

Positive

  • Low-Resistance Ohmic Contacts: Degenerate phosphorus doping (0.001–0.005 Ω·cm, ~10^19–10^20 cm^-3) enables metallic-like bulk conductivity for low-resistance backside ohmic contacts and conductive bottom gates in 200 mm device testing.
  • <111> Orientation for III-Nitride Epitaxy: The <111> crystal plane provides hexagonal three-fold surface symmetry and higher in-plane elastic modulus, supporting GaN-on-Si and III-nitride heteroepitaxy with slower wet alkaline etch kinetics than <100> silicon.

Trade-offs

  • High Doping Limits Thermal Budget: The degenerate phosphorus concentration (~10^19–10^20 cm^-3) can lead to dopant out-diffusion or autodoping during high-temperature epitaxy or oxidation steps, requiring careful thermal budget management.
  • <111> Orientation Etch Sensitivity: The <111> orientation exhibits slower wet alkaline etch kinetics and different surface chemistry than <100>, necessitating process re-optimization for cleaning, texturing, or anisotropic etching steps.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

5 pcs, 10 pcs, 25 pcs

Diameter

8-Inch (200.0 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

725 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)