8-Inch N-Type Silicon Wafer 100-1000 Ω·cm SSP ATOMFAIR®

Price range: $299.00 through $1,199.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 200 mm CZ N-type silicon wafer, 725 ± 25 μm, 100–1000 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 V-notch. In stock.

Diameter & Notch:
8-Inch (200.0 ± 0.2 mm)
SEMI V-Notch <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<100>•100–1000 Ω·cm
Thickness:
725 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Phosphorus-doped to 100–1000 Ω·cm, this high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, serving RF/microwave planar waveguides, IR/THz transmission windows (especially DSP), radiation/particle detector prototyping, and MEMS sensor isolation.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 8-Inch Notch & Precision

Standardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.

  • Diameter: 200.0 ± 0.2 mm (8.0 Inch)
  • Primary Fiducial: SEMI V-Notch along <110> ± 1° (Depth 1.0 +0.25/-0.00 mm, 90°)
  • Secondary Fiducial: None (SEMI M1 200 mm notch standard)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 200.0 ± 0.2 mm (8-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 725 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Fiducial (Notch) SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) SEMI M1 (200 mm)
Secondary Flat / Notch None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) SEMI M1 / Lot Laser ID
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes 200 mm Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • 200 mm Thin-Film Deposition & Stepper Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm, TTV < 5 μm) ensures uniform nucleation for epitaxy, PVD/CVD, ALD, and automated scanner lithography;
  • 200 mm CMOS, MEMS & Power Semiconductor Prototyping: Cleanroom <100> crystal plane supports KOH/TMAH anisotropic etching, Bosch DRIE, epitaxial growth, and pilot-line CMOS process integration;
  • 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (100–1000 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
  • In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 8-Inch (200 mm), N-Type (100), 100-1000 ohm-cm, 725 um, SSP (This Product) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type (100–1000 Ω·cm) SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, P-Type <100> Standard SEMI M1 200 mm notch CMOS & lithography substrate
8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) 8-Inch (200 mm) / DSP 725 ± 25 μm, P-Type <100> Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics
8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N-Type <100> Phosphorus-doped 200 mm wafer for power & CMOS R&D
8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) 8-Inch (200 mm) / SSP 725 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped 200 mm epi substrate

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon substrates require particulate-controlled storage and edge-only contact to preserve CMP surface integrity. Ambient native oxide growth and ionic contamination must be managed prior to downstream thermal or deposition processes.

  • Atmospheric Storage Control: Store wafers sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator to limit native oxide growth and airborne organic contamination.
  • Particulate and Vapor Isolation: Keep substrates away from particulate dust and corrosive vapors that degrade the mirror-polished front surface and introduce interface defects.
  • Edge-Only Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent scratching or contaminating the polished face.
  • Native Oxide Interface Awareness: Account for the ambient 1–2 nm native SiO2 layer when planning metallization, epitaxy, or ohmic contact formation on bare prime silicon.
  • Wet-Chemical EHS Compliance: Perform all RCA cleans, native oxide removal, and wet etching inside an exhaust fume hood or automated wet bench under institutional EHS and SDS protocols.

Sequential cleaning and surface conditioning steps preserve CMP cleanliness and reproducible thin-film interfaces on 200 mm prime silicon substrates. Each step must be executed under cleanroom conditions with facility-approved protocols.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, 200 mm cleanroom cassette or FOUP carrier, Exhaust fume hood or automated wet bench, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect Cassette and Wafer
    Inspect the sealed cleanroom cassette and wafer edges for particulate contamination or mechanical damage before opening.
  2. Transfer by Edge Contact
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease Sequentially
    Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water, or apply a megasonic SC-1 clean.
  4. Dry with Nitrogen
    Blow-dry the wafer with filtered N2 to remove residual solvent and water from the polished surface.
  5. Descum with Oxygen Plasma
    Apply a mild O2 plasma descum to remove residual organics prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove Native Oxide if Required
    Perform native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench when metallization or epitaxy demands an oxide-free interface.
  7. Return to Nitrogen Storage
    Return unused wafers to the original cleanroom cassette and store sealed within a dry nitrogen cabinet to minimize recontamination.

What is the resistivity range of this 8-inch N-type silicon wafer, and how does it affect RF and detector applications?

This wafer is Phosphorus-doped to a verified resistivity of 100–1000 Ω·cm, measured by four-point probe. The high-resistivity n-type CZ substrate suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar waveguides, IR/THz transmission windows, radiation/particle detector prototyping, and MEMS sensor isolation.

Is this 200 mm silicon wafer compatible with automated FOUP cassettes and cluster tools?

Yes. The wafer meets SEMI M1 specifications with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°). This geometry ensures reliable optical alignment and handling across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers.

How should I store and handle these prime-grade 8-inch silicon wafers to maintain surface cleanliness?

Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in 200 mm cleanroom protective cassettes (5, 10, or 25 pcs) that immobilize edges and prevent surface contact during transit.

The 8-inch prime CZ n-type silicon wafer with 100–1000 Ω·cm resistivity and SSP finish provides a high-resistivity, low-defect substrate suited for RF/microwave, detector, and MEMS prototyping, while its SEMI M1 geometry ensures compatibility with automated 200 mm tooling. However, successful integration requires cleanroom handling, native-oxide control, and strict wet-bench protocols to preserve surface quality.

Positive

  • High-Resistivity N-Type Substrate: Phosphorus doping at 100–1000 Ω·cm suppresses conductive substrate coupling and parasitic RF loss, making it suitable for RF/microwave planar waveguides and IR/THz transmission windows.
  • SEMI M1 200 mm Compatibility: Standard 200.0 mm diameter, V-notch fiducial, and 725 μm thickness enable direct use in automated FOUP cassettes, robotic cluster tools, lithography scanners, and CMP polishers.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 film; wet processing or RCA clean must be performed in an exhaust fume hood or automated wet bench to ensure ohmic interfaces.
  • Cleanroom Handling Mandatory: Wafers must be stored in dry nitrogen cabinets and handled only by perimeter edges with cleanroom tools to prevent particulate contamination and preserve the Ra < 0.5 nm surface.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

5 pcs, 10 pcs, 25 pcs

Diameter

8-Inch (200.0 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

725 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)