| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•10–20 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 10–20 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Phosphorus-doped to 10–20 Ω·cm (~2×1014–4.5×1014 cm-3 electron density), this moderate-resistivity n-type substrate minimizes ionized-impurity scattering and junction capacitance, supporting MOS capacitor gate metrology, photodiode arrays, and minority-hole lifetime studies.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm, TTV < 3 μm) supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding;
- 200 mm CMOS, MEMS & Power Semiconductor Prototyping: Cleanroom <100> crystal plane supports KOH/TMAH anisotropic etching, Bosch DRIE, epitaxial growth, and pilot-line CMOS process integration;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (10–20 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type (100), 10-20 ohm-cm, 725 um, DSP (This Product) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, N-Type (10–20 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade 200 mm silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Environmental exposure to particulates, corrosive vapors, and uncontrolled humidity must be avoided to prevent surface contamination and native oxide growth.
- Cleanroom Storage Requirements: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling Protocol: Handle wafers strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air that must be removed before metallization or epitaxy where ohmic interface control is required.
- Wet Processing Containment: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols.
- Cassette Immobilization: Keep unused wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier to minimize airborne organic contamination.
Proper handling and pre-cleaning of prime-grade 200 mm silicon wafers preserves CMP surface quality and ensures reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to photoresist coating or deposition.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet, O2 plasma descum system
- Inspect wafer cassette
Inspect the cleanroom protective cassette for edge damage or particulate contamination before opening. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease sequentially
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water or perform a megasonic/SC-1 clean. - Dry with nitrogen
Dry the wafer with a nitrogen blow-dry to remove residual solvent and water from the polished surfaces. - Apply plasma descum
Apply a mild O2 plasma descum to remove residual organic contamination prior to photoresist spin coating or PVD/ALD. - Remove native oxide if required
Remove the native oxide via RCA standard clean or wet processing inside an exhaust fume hood when ohmic interface control is required before metallization or epitaxy. - Store unused wafers
Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination.
What is the resistivity and dopant type of this 8-inch silicon wafer, and how does it affect device performance?
This wafer is N-type, Phosphorus-doped with a resistivity of 10–20 Ω·cm, corresponding to an electron density of approximately 2×10^14–4.5×10^14 cm^-3. This moderate resistivity minimizes ionized-impurity scattering and junction capacitance, making it suitable for MOS capacitor gate metrology, photodiode arrays, and minority-hole lifetime studies.
Is this wafer compatible with automated 200 mm fabrication tools such as FOUP cassettes and lithography scanners?
Yes. The wafer meets SEMI M1 standards with a diameter of 200.0 ± 0.2 mm, thickness of 725 ± 25 μm, and a SEMI V-notch along <110> ± 1° (depth 1.0 mm, 90°). This geometry ensures reliable handling in automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers.
How should these prime silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or with robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers. The wafers are supplied in 200 mm cleanroom protective cassettes (5, 10, or 25 pcs) that immobilize edges and prevent surface contact during transit.
The 8-inch prime CZ N-type <100> silicon wafer with 10–20 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a well-characterized substrate for 200 mm CMOS/MEMS prototyping, double-side lithography, and in-house oxidation. Its SEMI M1 geometry and tight TTV/bow/warp tolerances support automated FOUP handling, but deployment requires cleanroom infrastructure and strict wet-bench protocols to preserve surface quality.
Positive
- Dual-Side CMP for Bonding and Lithography: Double-side polished surfaces with Ra < 0.5 nm and TTV < 3 μm enable double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding with reproducible thin-film growth.
- SEMI M1 Geometry for Automated Tools: Standardized 200.0 ± 0.2 mm diameter, SEMI V-notch along <110>, and 725 ± 25 μm thickness ensure reliable alignment and transport across FOUP cassettes, robotic cluster tools, lithography scanners, and CMP polishers.
Trade-offs
- Cleanroom Handling Required: Bare prime silicon must be handled strictly by perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers; exposure to particulate dust or corrosive vapors degrades the CMP surface.
- Native Oxide and Wet-Bench Dependency: An ambient ~1–2 nm native SiO2 film forms in air, requiring RCA standard clean or wet processing inside an exhaust fume hood or automated wet bench under institutional EHS and SDS protocols before metallization or epitaxy.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).