| Diameter & Notch: 8-Inch (200.0 ± 0.2 mm) SEMI V-Notch <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.01–0.1 Ω·cm |
Thickness: 725 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
8-Inch (200 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 200.0 ± 0.2 mm diameter and 725 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+) (~1017–5×1018 cm-3 donor concentration), the wafer combines low substrate series resistance with lower free-carrier IR optical absorption than N++ substrates, supporting vertical diodes, anodic bonding, and working electrodes.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
8-Inch (200 mm) Thickness & Tool Compatibility Note: The SEMI M1 standard 725 ± 25 μm mechanical thickness offers high flexural stiffness across automated 200 mm FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible 200 mm thin-film growth and lithography.
|
SEMI M1 8-Inch Notch & PrecisionStandardized 200.0 mm diameter and precision SEMI V-notch fiducial ensure reliable optical alignment across automated FOUP handlers, steppers, and cleanroom cluster tools.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 200.0 ± 0.2 mm (8-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 725 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Fiducial (Notch) | SEMI V-Notch along <110> ± 1°•Depth: 1.0 mm (90° angle) | SEMI M1 (200 mm) |
| Secondary Flat / Notch | None (Standard 200 mm SEMI M1 single-notch wafer; type & orientation documented on CoA) | SEMI M1 / Lot Laser ID |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 5 pcs, 10 pcs, 25 pcs cleanroom protective cassettes | 200 mm Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- 200 mm Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm, TTV < 3 μm) supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion/anodic bonding;
- 200 mm CMOS, MEMS & Power Semiconductor Prototyping: Cleanroom <100> crystal plane supports KOH/TMAH anisotropic etching, Bosch DRIE, epitaxial growth, and pilot-line CMOS process integration;
- 200 mm Semiconductor & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and automated C-V metrology;
- In-House Oxidation & Process Qualification: Virgin prime wafer for custom vertical-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and tool calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in 200 mm cleanroom protective cassettes (5 pcs, 10 pcs, 25 pcs options) engineered to immobilize wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge or robotic end-effectors using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, TTV/bow/warp, crystal orientation, and cleanroom particle inspection criteria, with institutional compliance documentation available on request.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 8-Inch (200 mm), N-Type (100), 0.01-0.1 ohm-cm, 725 um, DSP (This Product) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, N-Type (0.01–0.1 Ω·cm) | SEMI M1 200 mm notch wafer in 5 / 10 / 25 pcs cassettes |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, P-Type <100> | Standard SEMI M1 200 mm notch CMOS & lithography substrate |
| 8-Inch P-Type <100> Wafer (1–10 Ω·cm, 725 μm DSP) | 8-Inch (200 mm) / DSP | 725 ± 25 μm, P-Type <100> | Double-side CMP (TTV < 3 μm) for 200 mm bonding & IR optics |
| 8-Inch N-Type <100> Wafer (1–10 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N-Type <100> | Phosphorus-doped 200 mm wafer for power & CMOS R&D |
| 8-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 725 μm SSP) | 8-Inch (200 mm) / SSP | 725 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped 200 mm epi substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 8-inch wafers sequentially in electronic-grade acetone, isopropanol (IPA), and DI water (or megasonic/SC-1 clean), followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or automated wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused 200 mm wafers sealed inside the original cleanroom polypropylene cassette or FOUP carrier within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom handling to preserve CMP surface quality and prevent particulate contamination. Storage must occur in sealed nitrogen environments to minimize native oxide growth and airborne organic contamination.
- Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge or with cleanroom vacuum wands and PTFE/PEEK tweezers to avoid surface contact and particle deposition.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled removal before metallization or epitaxial growth.
- Atmospheric Storage Requirements: Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Wet Processing Safety: All wet-chemical or cleanroom processing must follow institutional EHS and SDS safety protocols within exhaust fume hoods or automated wet benches.
Proper handling and pre-cleaning procedures preserve the CMP mirror finish and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the surface for photoresist or deposition processes.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, 200 mm cleanroom cassette or FOUP carrier, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or automated wet bench
- Inspect wafer packaging
Verify the cleanroom cassette seal is intact and inspect wafers for visible particulate contamination under bright light before opening. - Transfer wafer with edge handling
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers, handling strictly by the perimeter edge to avoid surface contact. - Perform solvent pre-cleaning
Degrease the wafer sequentially in electronic-grade acetone, isopropanol, and DI water, or use megasonic/SC-1 clean as appropriate. - Dry and descum surface
Blow-dry with nitrogen and apply mild oxygen plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or automated wet bench using facility-approved protocols. - Store unused wafers properly
Return unused wafers to the original cleanroom cassette and store sealed within a dry nitrogen cabinet to minimize contamination.
What is the resistivity and dopant concentration of this 8-inch N-type silicon wafer?
This wafer is Phosphorus-doped N-type with a verified resistivity of 0.01–0.1 Ω·cm, corresponding to a donor concentration of approximately 10^17–5×10^18 cm^-3. The low-resistivity range provides low substrate series resistance while maintaining lower free-carrier IR absorption than N++ substrates, making it suitable for vertical diodes, anodic bonding, and working electrodes.
Is this wafer compatible with automated 200 mm FOUP cassettes and cluster tools?
Yes. The wafer meets SEMI M1 specifications with a 200.0 ± 0.2 mm diameter, 725 ± 25 μm thickness, and a SEMI V-Notch along <110> ± 1° (depth 1.0 mm, 90°). This geometry ensures reliable optical alignment and handling across automated FOUP cassettes, robotic cluster tools, lithography scanners, CMP polishers, and RTP chambers.
How should these prime silicon wafers be stored and handled to maintain surface quality?
Store wafers sealed in their original cleanroom protective cassettes inside a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the dual-side mirror-polished surfaces (Ra < 0.5 nm).
The 8-inch N-type prime CZ silicon wafer with 0.01–0.1 Ω·cm resistivity and DSP finish offers a low-resistance, low-absorption substrate for vertical diodes, anodic bonding, and double-side lithography, while its SEMI M1 geometry ensures compatibility with automated 200 mm tooling. However, successful use requires cleanroom handling, native oxide control, and strict wet-chemistry safety protocols.
Positive
- Low resistivity, low IR absorption: Phosphorus doping at 0.01–0.1 Ω·cm provides low substrate series resistance while maintaining lower free-carrier IR absorption than N++ substrates, benefiting vertical diodes and working electrodes.
- Dual-side mirror polish for bonding: Double-side CMP with Ra < 0.5 nm and TTV < 3 μm supports double-sided MEMS patterning, through-wafer IR transmission, and automated fusion or anodic bonding.
Trade-offs
- Native oxide requires removal: Bare prime silicon forms a 1–2 nm native SiO2 film in air; removal before metallization or epitaxy requires wet processing in an exhaust fume hood or automated wet bench under institutional EHS protocols.
- Cleanroom handling mandatory: To preserve CMP cleanliness and prevent particle contamination, wafers must be stored in dry nitrogen cabinets and handled only with cleanroom vacuum wands or PTFE/PEEK tweezers by the perimeter edge.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.