6-Inch N-Type Silicon Wafer 20-50 Ω·cm SSP ATOMFAIR®

Price range: $329.00 through $729.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 150 mm CZ N-type silicon wafer, 675 μm, 20–50 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•20–50 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 20–50 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to 20–50 Ω·cm (~9×1013–2×1014 cm-3 donor concentration), this low-doping n-type substrate widens depletion layers and reduces parasitic capacitance for PIN optical/particle photodetectors, high-voltage sensor diodes, and low-noise analog test structures.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 37.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 150 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 20–50 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat 37.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 150 mm N<111>) SEMI M1 (150 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Phosphorus-doped (20–50 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), N-Type (111), 20-50 ohm-cm, 675 um, SSP (This Product) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type (20–50 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N-Type <100> Standard SEMI M1 675 μm 150 mm N-type lithography substrate
6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, N-Type <100> Double-side CMP polished N-type 150 mm wafer for bonding & IR
6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N++ As <100> Low-strain, low-diffusivity As-doped epi & MOSFET substrate
6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, N+ Sb <100> Minimal autodoping Sb-doped wafer for sharp high-T epitaxy

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve the CMP-polished surface. Ambient native oxide growth and particulate contamination must be controlled prior to any thin-film or lithographic processing.

  • Native Oxide Formation: Bare prime silicon forms an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed prior to metallization or epitaxy where an oxide-free interface is required.
  • Particulate and Organic Contamination Control: Unused wafers must remain sealed in the original cleanroom polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic and particulate contamination.
  • Edge-Only Handling Requirement: Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the mirror-polished front surface.
  • Corrosive Vapor and Dust Exposure: Storage away from particulate dust and corrosive vapors is required to prevent surface degradation of the SSP finish.
  • Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols, with native oxide removal or RCA standard cleans performed inside an exhaust fume hood or wet bench.

Proper handling preserves the CMP-polished surface and ensures reproducible thin-film interfaces. Sequential solvent cleaning, plasma descum, and controlled storage are required prior to lithography or deposition.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect Cassette and Wafer Edges
    Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before removing any wafer.
  2. Transfer Wafer by Perimeter Edge
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied strictly to the perimeter edge.
  3. Degrease in Solvent Sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry and Descum Surface
    Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove Native Oxide Under Hood
    Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols where an oxide-free interface is required.
  6. Store Unused Wafers Sealed
    Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet.

Why choose a <111> orientation N-type silicon wafer over <100> for epitaxy or sensor fabrication?

The <111> orientation provides a densely packed three-fold surface symmetry with a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon. Combined with the 20–50 Ω·cm phosphorus doping (~9×10^13–2×10^14 cm^-3), this widens depletion layers and reduces parasitic capacitance, making it suited for PIN optical/particle photodetectors, high-voltage sensor diodes, and lattice-matched GaN/AlN/SiC heteroepitaxy. If your process instead requires standard <100> lithography or anisotropic KOH etching, a <100> wafer is the appropriate choice.

Can this 6-inch SSP wafer be processed directly in a 150 mm stepper and LPCVD/PECVD line without additional preparation?

Yes. The 675 ± 25 μm SEMI M1 thickness and 150.0 ± 0.3 mm diameter provide the flexural stiffness and dimensional registration required by automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. The primary flat is 57.5 ± 2.5 mm along <110> ± 1° with a 37.5 ± 2.5 mm secondary flat at 45° ± 5° clockwise (SEMI M1 150 mm N<111>), ensuring correct cassette and FOUP alignment. The bare prime surface carries only a ~1–2 nm native oxide, so in-house thermal oxidation, wet etching, or epitaxial growth can proceed directly.

How should these prime silicon wafers be stored and handled to preserve the Ra < 0.5 nm CMP surface?

Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the mirror-polished front surface (SSP, Ra < 0.5 nm). For pre-cleaning, degrease sequentially in acetone, electronic-grade IPA, and DI water, follow with N2 blow-drying and a mild O2 plasma descum before photoresist spin coating or PVD/ALD; any wet-chemical processing must follow institutional EHS and SDS protocols.

The 6-inch N-type <111> prime silicon wafer with 20–50 Ω·cm resistivity and SSP finish offers a low-doped, crystallographically oriented substrate suited for hexagonal epitaxy, high-voltage sensor diodes, and low-noise analog test structures. Its SEMI M1-compliant 675 μm thickness and cleanroom cassette packaging support automated 150 mm processing, though users must account for native oxide formation and strict cleanroom handling to preserve surface quality.

Positive

  • Low-Doped N-Type for Wide Depletion: Phosphorus doping at 20–50 Ω·cm widens depletion layers and reduces parasitic capacitance, benefiting PIN photodetectors, high-voltage sensor diodes, and low-noise analog test structures.
  • <111> Orientation for Hexagonal Epitaxy: The densely packed <111> plane provides three-fold surface symmetry and slower wet alkaline etch kinetics, supporting III-nitride heteroepitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies.

Trade-offs

  • Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film in air; wet processing or RCA clean is necessary before metallization or epitaxy, requiring exhaust fume hood or wet bench facilities.
  • Cleanroom Handling Mandatory: To preserve CMP surface quality (Ra < 0.5 nm) and prevent particulate contamination, wafers must be stored in dry nitrogen cabinets and handled only with cleanroom vacuum wands or PTFE/PEEK tweezers.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

20-50 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)