| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <111>•0.001–0.005 Ω·cm |
Thickness: 675 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Degenerately Phosphorus-doped to 0.001–0.005 Ω·cm (N++) (~1019–1020 cm-3 electron density), the wafer delivers metallic-like bulk conductivity for low-resistance backside ohmic contacts, conductive bottom gates, III-V/GaN buffer heteroepitaxy, and high-current device testing.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.001–0.005 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 675 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 150 mm N<111>) | SEMI M1 (150 mm N<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Phosphorus-doped (0.001–0.005 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), N-Type (111), 0.001-0.005 ohm-cm, 675 um, SSP (This Product) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N-Type (0.001–0.005 Ω·cm) | SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N-Type <100> | Standard SEMI M1 675 μm 150 mm N-type lithography substrate |
| 6-Inch N-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, N-Type <100> | Double-side CMP polished N-type 150 mm wafer for bonding & IR |
| 6-Inch N-Type Arsenic <100> Wafer (0.001–0.005 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N++ As <100> | Low-strain, low-diffusivity As-doped epi & MOSFET substrate |
| 6-Inch N-Type Antimony <100> Wafer (0.005–0.02 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, N+ Sb <100> | Minimal autodoping Sb-doped wafer for sharp high-T epitaxy |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve CMP surface quality. Ambient native oxide growth and particulate contamination must be controlled prior to lithography or epitaxy.
- Cleanroom Storage Atmosphere: Store sealed wafers inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air that must be removed before metallization or epitaxy where an ohmic interface is required.
- Wet Processing Containment: Perform all wet-chemical or RCA cleaning strictly inside an exhaust fume hood or wet bench using facility-approved EHS and SDS protocols.
- Cassette Immobilization: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box to minimize airborne organic contamination.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage to maintain wafer surface integrity.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench
- Inspect cassette seal
Verify the cleanroom cassette remains sealed and the wafer edges are immobilized before opening in a controlled environment. - Transfer by edge
Transfer wafers strictly by the perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers. - Degrease sequentially
Degrease wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry and descum
Blow-dry with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove native oxide
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols where ohmic interfaces are required. - Store sealed
Return unused wafers to the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
Why choose a <111> orientation N++ silicon wafer instead of <100> for GaN or AlN epitaxy?
The <111> plane provides hexagonal three-fold surface symmetry that better accommodates lattice-matched III-nitride heteroepitaxy (GaN, AlN, SiC) compared to <100> silicon. This wafer is oriented to <111> ± 0.5° and degenerately phosphorus-doped to 0.001–0.005 Ω·cm, delivering metallic-like bulk conductivity for low-resistance backside ohmic contacts and conductive bottom gates. The denser <111> plane also exhibits higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon.
Can this 675 µm thick 150 mm N++ wafer be processed on standard automated 150 mm photolithography and CVD tools?
Yes. The 675 ± 25 µm thickness conforms to the SEMI M1 standard for 150 mm wafers, providing high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. The 150.0 ± 0.3 mm diameter and SEMI M1 crystal alignment flats (57.5 ± 2.5 mm primary flat along <110> ± 1°, 37.5 ± 2.5 mm secondary flat at 45° ± 5° clockwise) ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
What surface preparation is required before epitaxy or metallization on this bare prime silicon wafer?
Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, so native oxide removal or an RCA standard clean is required before metallization or epitaxy. Perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols, following institutional EHS and SDS safety guidelines. For pre-cleaning, degrease sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
The 6-inch N-type <111> prime silicon wafer with 0.001–0.005 Ω·cm phosphorus doping and SSP finish provides a low-resistivity, crystallographically oriented substrate suited for III-nitride heteroepitaxy, ohmic contact formation, and high-current device prototyping. Its SEMI M1 geometry and 675 μm thickness ensure compatibility with automated 150 mm cleanroom tooling, though the <111> orientation and degenerate doping impose specific constraints on etch behavior and thermal budget management.
Positive
- Low-Resistivity N++ Ohmic Contacts: Phosphorus doping at 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3) enables metallic-like bulk conductivity for low-resistance backside ohmic contacts and conductive bottom gates.
- <111> Lattice for Hexagonal Epitaxy: The <111> (± 0.5°) orientation provides three-fold surface symmetry and higher in-plane elastic modulus, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
Trade-offs
- <111> Orientation Etch Sensitivity: Slower wet alkaline etch kinetics than <100> silicon requires adjusted etch recipes and may complicate standard anisotropic etching processes.
- Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film, necessitating RCA clean or wet processing in an exhaust fume hood before metallization or epitaxy.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).