| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•10–20 Ω·cm |
Thickness: 675 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 675 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | None (SEMI M1 standard for 150 mm P-type <111>) | SEMI M1 (150 mm P<111>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete power/bipolar prototyping;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), P-Type (111), 10-20 ohm-cm, 675 um, DSP (This Product) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type (10–20 Ω·cm) | SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <100> | Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type <100> | Double-side CMP polished 150 mm wafer for bonding & IR optics |
| 6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <111> | Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D |
| 6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & <110> hole-mobility wafer |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate, organic, and metallic contamination. Storage and handling must preserve the CMP mirror finish and prevent surface contact.
- Atmospheric Storage: Store sealed wafers inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Surface Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the dual-side polished surfaces.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by wet processing before metallization or epitaxy if an oxide-free interface is required.
- Wet Processing Environment: Perform all wet-chemical cleaning, native oxide removal, or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols.
- Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Proper handling and pre-cleaning preserve the CMP mirror finish and ensure reproducible thin-film interfaces. All wet-chemical processing must follow institutional EHS and SDS safety protocols.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet
- Inspect Cassette Seal
Verify the cleanroom protective cassette is sealed and undamaged before opening in a controlled environment. - Transfer Wafer
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease Surface
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water. - Dry Wafer
Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD. - Remove Native Oxide
Perform native oxide removal or RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols when an oxide-free interface is required. - Store Unused Wafers
Return unused wafers to the original cleanroom polypropylene cassette box and store inside a dry nitrogen cabinet.
Why choose a <111> orientation 6-inch silicon wafer over <100> for epitaxy or power device R&D?
The <111> orientation provides a densely packed three-fold surface symmetry with a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon. This makes it preferable for lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, UHV surface reconstruction studies, and discrete power/bipolar prototyping. In contrast, <100> wafers are typically chosen for standard CMOS lithography and KOH-based MEMS, where faster etch rates and different surface chemistry are advantageous.
What are the resistivity and dopant specifications of this 6-inch P-type <111> prime silicon wafer?
This wafer is Boron-doped (P-type) to a verified resistivity of 10–20 Ω·cm, corresponding to a dopant density of approximately 10^15 cm^-3. The moderate resistivity minimizes impurity scattering and junction capacitance compared to heavily doped wafers, making it suitable for MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures. Resistivity is measured by four-point probe (4PP) and documented on the Certificate of Analysis.
How should I handle and store these DSP prime silicon wafers to maintain surface quality?
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the dual-side mirror-polished surfaces (Ra < 0.5 nm). Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. For pre-cleaning, degrease sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
The 6-inch P-type <111> prime CZ silicon wafer with 10–20 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is engineered for hexagonal epitaxy, double-side lithography, and UHV surface physics, where the dense three-fold lattice and moderate doping reduce impurity scattering and junction capacitance. Its SEMI M1 675 μm thickness ensures mechanical compatibility with automated 150 mm tooling, but successful deployment requires cleanroom handling, native oxide control, and strict wet-bench protocols to preserve the pristine surface.
Positive
- Hexagonal Lattice for Epitaxy: The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies. Its higher in-plane elastic modulus and slower wet alkaline etch kinetics compared to <100> silicon offer advantages for discrete power and bipolar R&D.
- Dual-Side CMP Finish: Double-side mirror-polished surfaces with Ra < 0.5 nm enable double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The sub-nanometer roughness ensures reproducible thin-film growth and lithography.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, which must be removed via wet processing (e.g., RCA clean or HF dip) before metallization or epitaxy. This step requires an exhaust fume hood or wet bench and strict adherence to institutional EHS and SDS protocols.
- Cleanroom Handling Mandatory: To preserve the CMP surface and prevent particulate contamination, wafers must be stored in a dry nitrogen cabinet or cleanroom desiccator and handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers. Unsealed exposure to airborne organics can degrade surface quality.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).