| Diameter & Flat: 6-Inch (150.0 ± 0.3 mm) Primary Flat 57.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•100–1000 Ω·cm |
Thickness: 675 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 6-Inch Dimensional PrecisionStandardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 100–1000 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 150.0 ± 0.3 mm (6-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 675 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 57.5 ± 2.5 mm | SEMI M1 (150 mm) |
| Secondary Flat | 37.5 ± 2.5 mm secondary flat at 90° ± 5° clockwise (or single-flat SEMI 150 mm per batch CoA) | SEMI M1 (150 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
- Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 6-Inch (150 mm), P-Type (100), 100-1000 ohm-cm, 675 um, DSP (This Product) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type (100–1000 Ω·cm) | SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <100> | Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate |
| 6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) | 6-Inch (150 mm) / DSP | 675 ± 25 μm, P-Type <100> | Double-side CMP polished 150 mm wafer for bonding & IR optics |
| 6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <111> | Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D |
| 6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) | 6-Inch (150 mm) / SSP | 675 ± 25 μm, P-Type <110> | Vertical-sidewall KOH MEMS & <110> hole-mobility wafer |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve CMP surface quality and prevent particulate contamination. Environmental exposure to airborne organics, moisture, and corrosive vapors degrades the native oxide interface and lithographic reproducibility.
- Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact and particle transfer.
- Storage Atmosphere Requirements: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled wet processing before metallization or epitaxy where oxide-free interfaces are needed.
- Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols within exhaust fume hoods or wet benches.
Proper handling preserves the dual-side CMP mirror finish and ensures reproducible thin-film interfaces across cleanroom processing runs. Sequential solvent cleaning and controlled storage minimize organic and particulate contamination.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet, Cleanroom polypropylene cassette
- Inspect Cassette Seal
Verify the cleanroom cassette seal is intact and confirm the wafer count matches the Certificate of Analysis before opening. - Transfer Wafer by Edge
Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease in Solvent Sequence
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water followed by N2 blow-drying. - Apply Plasma Descum
Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Perform Wet Processing in Hood
Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols. - Return to Nitrogen Storage
Return unused wafers to the original cleanroom polypropylene cassette and store within a dry nitrogen cabinet.
What is the resistivity range of this 6-inch P-type <100> silicon wafer, and how does it affect RF and photodetector performance?
This wafer is Boron-doped to a verified resistivity of 100–1000 Ω·cm, measured by four-point probe (4PP). The high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation. The <100> (± 0.5°) crystal orientation is confirmed by X-ray diffraction (XRD).
Is this 150 mm prime silicon wafer compatible with KOH or TMAH anisotropic etching for MEMS fabrication?
Yes. The <100> (± 0.5°) crystal plane supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions, as well as Bosch DRIE and epitaxial layer growth. The cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, and the low Si/SiO2 interface state density supports MEMS, CMOS, and power device prototyping.
How should these DSP prime silicon wafers be stored and handled to preserve the Ra < 0.5 nm CMP surface?
Wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs) engineered to immobilize 6-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors, and handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), so keep unused wafers sealed in the original polypropylene cassette box to minimize airborne organic contamination.
The 6-inch prime CZ P-type <100> silicon wafer with 100–1000 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a high-resistivity substrate optimized for RF/microwave, THz/IR optics, and MEMS isolation, where suppressed free-carrier loss and parasitic capacitance are critical. Its SEMI M1 675 μm thickness and <100> orientation ensure compatibility with automated 150 mm lithography, epitaxy, and KOH/TMAH anisotropic etching, though the bare surface requires strict cleanroom handling and immediate native-oxide management.
Positive
- High-Resistivity Suppresses Conductive Loss: Boron-doped to 100–1000 Ω·cm, this substrate minimizes free-carrier absorption and parasitic capacitance, directly benefiting RF/microwave coplanar waveguides, THz/IR windows, and photodetector isolation.
- Dual-Side CMP Enables Bonding and IR: Double-side mirror polish (Ra < 0.5 nm) supports double-sided lithography, through-wafer IR transmission, and direct fusion/anodic bonding without additional surface preparation.
Trade-offs
- Native Oxide Requires Removal Before Metallization: Bare prime silicon forms a 1–2 nm ambient native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench to ensure ohmic interfaces before epitaxy or metallization.
- Strict Cleanroom Handling Mandatory: To preserve CMP cleanliness and prevent particulate contamination, wafers must be stored in a dry nitrogen cabinet and handled only by the perimeter edge using vacuum wands or PTFE/PEEK tweezers.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).