6-Inch Prime CZ Silicon Wafer P-Type 100-1000 Ω·cm ATOMFAIR®

Price range: $289.00 through $629.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 150 mm CZ P-type silicon wafer, 675 ± 25 μm, 100–1000 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
6-Inch (150.0 ± 0.3 mm)
Primary Flat 57.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•100–1000 Ω·cm
Thickness:
675 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

6-Inch (150 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 150.0 ± 0.3 mm diameter and 675 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

6-Inch (150 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 675 ± 25 μm mechanical thickness offers high flexural stiffness across automated 150 mm photolithography steppers, PECVD/LPCVD cassettes, epitaxial susceptors, and robotic handling chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 6-Inch Dimensional Precision

Standardized 150.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers.

  • Diameter: 150.0 ± 0.3 mm (6.0 Inch)
  • Primary Flat: 57.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 37.5 ± 2.5 mm secondary flat at 90° ± 5° clockwise (or single-flat SEMI 150 mm per batch CoA)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 150.0 ± 0.3 mm (6-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 675 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 57.5 ± 2.5 mm SEMI M1 (150 mm)
Secondary Flat 37.5 ± 2.5 mm secondary flat at 90° ± 5° clockwise (or single-flat SEMI 150 mm per batch CoA) SEMI M1 (150 mm P<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for epitaxy, PVD sputtering, ALD, and high-resolution 150 mm stepper lithography;
  • MEMS, CMOS & Power Device Prototyping: Cleanroom <100> crystal plane supports KOH / TMAH anisotropic etching, Bosch DRIE, epitaxial layer growth, and pilot-line CMOS fabrication;
  • Semiconductor Device & Pilot-Line Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, power/RF devices, epitaxial growth, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 6-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, dopants, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 6-Inch (150 mm), P-Type (100), 100-1000 ohm-cm, 675 um, SSP (This Product) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type (100–1000 Ω·cm) SEMI M1 675 μm 150 mm wafer in 10 pcs / 25 pcs cassettes
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <100> Standard SEMI M1 675 μm 150 mm lithography & CMOS substrate
6-Inch P-Type <100> Wafer (1–10 Ω·cm, 675 μm DSP) 6-Inch (150 mm) / DSP 675 ± 25 μm, P-Type <100> Double-side CMP polished 150 mm wafer for bonding & IR optics
6-Inch P-Type <111> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <111> Hexagonal <111> 150 mm lattice for heteroepitaxy & power R&D
6-Inch P-Type <110> Wafer (1–10 Ω·cm, 675 μm SSP) 6-Inch (150 mm) / SSP 675 ± 25 μm, P-Type <110> Vertical-sidewall KOH MEMS & <110> hole-mobility wafer

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 6-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom handling to prevent particulate contamination and surface damage. Storage must be in a dry nitrogen cabinet or cleanroom desiccator away from corrosive vapors.

  • Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact.
  • Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed before metallization or epitaxy if an ohmic interface is required.
  • Storage Environment: Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.

Proper handling and pre-cleaning steps are essential to preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. These steps outline the recommended sequence for degreasing, native oxide control, and storage.

Required Equipment: Cleanroom vacuum wands or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect wafer cassette
    Inspect the cleanroom protective cassette for any signs of damage or particulate contamination before opening.
  2. Handle wafer by edge
    Handle the wafer strictly by its perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
  3. Degrease wafer surface
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water, followed by N2 blow-drying.
  4. Perform plasma descum
    Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  5. Remove native oxide if required
    Remove the native oxide via RCA standard clean or wet processing inside an exhaust fume hood or wet bench using facility-approved protocols.
  6. Store unused wafers
    Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.

What is the resistivity range of this 6-inch P-type <100> silicon wafer, and how does it affect RF/microwave device performance?

This wafer is Boron-doped to a verified resistivity of 100–1000 Ω·cm, as measured by four-point probe (4PP). This high-resistivity range substantially suppresses free-carrier conductive loss and parasitic capacitance, making the substrate well suited for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation. The lightly doped CZ monocrystalline silicon provides a controlled base for ohmic contacts and C-V metrology in device prototyping.

Can this SSP wafer be used for double-side processing or bonding applications that require a polished back surface?

No. This product is single-side polished (SSP) with a mirror-polished front surface (Ra < 0.5 nm) and a fine-ground back surface. For applications requiring double-side polishing (DSP), such as wafer bonding or IR optics, a separate DSP variant is available. The fine-ground back surface of this SSP wafer is not suitable for direct bonding or backside lithography without additional preparation.

What cleanroom handling and storage procedures are required to maintain the surface quality of this prime silicon wafer?

Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and store them sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors. The bare prime silicon surface carries only a thin ambient native oxide (~1–2 nm), so solvent pre-cleaning (acetone, IPA, DI water) followed by N2 blow-drying and mild O2 plasma descum is recommended before photoresist spin coating or PVD/ALD. All wet-chemical processing must follow institutional EHS and SDS safety protocols.

This 6-inch prime CZ P-type <100> silicon wafer with 100–1000 Ω·cm resistivity and SSP finish (Ra < 0.5 nm) is engineered for high-resistivity RF/microwave, THz/IR optical, and MEMS isolation applications where free-carrier loss and parasitic capacitance must be minimized. Its SEMI M1-compliant 675 μm thickness and <100> orientation support standard 150 mm lithography, KOH/TMAH anisotropic etching, and in-house thermal oxidation, though bare-surface handling and cleanroom storage are mandatory to preserve the CMP finish.

Positive

  • High-Resistivity Substrate for RF and Optical Use: Boron-doped to 100–1000 Ω·cm, this CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation.
  • SEMI M1 Geometry for Automated 150 mm Tools: The 150.0 ± 0.3 mm diameter, 675 ± 25 μm thickness, and <110> primary flat ensure accurate registration on vacuum chucks, mask aligners, and cleanroom FOUP/cassette carriers, with high flexural stiffness across automated photolithography steppers and epitaxial susceptors.

Trade-offs

  • Bare Surface Requires Strict Cleanroom Handling: The SSP CMP finish (Ra < 0.5 nm) is uncoated and vulnerable to particulate and organic contamination; wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or desiccator.
  • Native Oxide Necessitates Wet Processing Infrastructure: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; where native oxide removal or RCA standard clean is required before metallization or epitaxy, wet processing must be performed inside an exhaust fume hood or wet bench using facility-approved protocols.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

6-Inch (150.0 ± 0.3 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

675 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)