Prime CZ N-Type silicon wafer, 125.0 ± 0.5 mm, 625 ± 25 μm, 10–20 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
5-Inch (125.0 ± 0.5 mm)
Primary Flat 42.5 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•10–20 Ω·cm
Thickness:
625 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Phosphorus-doped to 10–20 Ω·cm (~2×1014–4.5×1014 cm-3 electron density), this moderate-resistivity n-type substrate minimizes ionized-impurity scattering and junction capacitance, supporting MOS capacitor gate metrology, photodiode arrays, and minority-hole diffusion lifetime studies.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 5-Inch Dimensional Precision

Standardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 125.0 ± 0.5 mm (5.0 Inch)
  • Primary Flat: 42.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 27.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 125 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 10–20 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 125.0 ± 0.5 mm (5-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 625 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 42.5 ± 2.5 mm SEMI M1 (125 mm)
Secondary Flat 27.5 ± 2.5 mm secondary flat located 45° ± 5° clockwise from primary flat (SEMI M1 125 mm N<111>) SEMI M1 (125 mm N<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 5-Inch (125 mm), N-Type (111), 10-20 ohm-cm, 625 um, SSP (This Product) 5-Inch (125 mm) / SSP 625 ± 25 μm, N-Type (10–20 Ω·cm) SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <100> Standard SEMI M1 625 μm 125 mm P-type lithography substrate
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) 5-Inch (125 mm) / DSP 625 ± 25 μm, P-Type <100> Double-side CMP polished 125 mm wafer for IR optics & bonding
5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, N-Type <100> Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D
5-Inch P-Type <111> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <111> Hexagonal <111> 125 mm lattice for heteroepitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only contact to preserve the CMP-polished surface. Ambient native oxide growth and ionic contamination must be managed before any thermal or epitaxial processing.

  • Particulate and Organic Contamination Control: Store wafers sealed in the original cleanroom cassette inside a dry nitrogen cabinet or desiccator to limit airborne organic and particulate contamination.
  • Edge-Only Contact Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished front surface.
  • Native Oxide Sensitivity: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed by RCA clean or wet processing before metallization or epitaxy.
  • Corrosive Vapor and Dust Exposure: Keep wafers away from particulate dust and corrosive vapors that can degrade surface quality and compromise thin-film nucleation.
  • Wet-Chemical Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

Proper handling preserves the mirror-polished CMP surface and prevents contamination during device fabrication. Sequential solvent cleaning and native oxide control are required before photoresist spin coating or thin-film deposition.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet

  1. Inspect cassette and wafer
    Inspect the cleanroom cassette and wafer edges for particulate contamination or physical damage before opening.
  2. Transfer wafer by edge
    Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease in solvent sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic residues.
  4. Dry with nitrogen
    Dry the wafer with a nitrogen blow-dry to remove residual solvent and water from the polished surface.
  5. Descum with oxygen plasma
    Apply a mild oxygen plasma descum to remove trace organics prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove native oxide if required
    Perform RCA standard clean or wet oxide removal inside an exhaust fume hood when native oxide removal is required before metallization or epitaxy.
  7. Store unused wafers sealed
    Store unused wafers sealed inside the original cleanroom cassette within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a <111> N-type silicon wafer over <100> for epitaxy or device prototyping?

The <111> orientation provides a densely packed three-fold surface symmetry with a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon. This makes it preferable for lattice-matched III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D. The phosphorus-doped 10–20 Ω·cm bulk resistivity further minimizes ionized-impurity scattering and junction capacitance for MOS capacitor gate metrology and minority-hole diffusion lifetime studies.

Is the 625 µm thickness of this 5-inch wafer compatible with standard diffusion tube boats and PECVD/LPCVD cassettes?

Yes. The 625 ± 25 µm thickness conforms to the SEMI M1 standard for 125 mm wafers, providing high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. The 125.0 ± 0.5 mm diameter and SEMI M1 crystal alignment flats (42.5 ± 2.5 mm primary flat along <110> ± 1°) ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

How should bare prime silicon wafers be stored and handled to preserve the CMP surface before thermal oxidation or epitaxy?

Store wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the mirror-polished front surface (Ra < 0.5 nm). Bare prime silicon carries only a thin ambient native oxide (~1–2 nm); where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols.

The 5-inch N-type <111> prime CZ silicon wafer with 10–20 Ω·cm resistivity and SSP finish offers a lattice-matched platform for hexagonal epitaxy and MOS metrology, but its <111> orientation and bare surface demand orientation-specific process tuning and strict cleanroom handling to avoid contamination and native oxide interference.

Positive

  • Hexagonal Lattice for Epitaxy: The <111> crystal orientation provides three-fold surface symmetry and a densely packed plane, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
  • Low-Defect CMP Surface: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, and high-resolution photoresist spin coating, while the fine-ground back aids handling.

Trade-offs

  • <111> Orientation Process Sensitivity: The <111> plane exhibits slower wet alkaline etch kinetics than <100> silicon, requiring orientation-specific etch recipes and potentially longer process times for micromachining or cleaning steps.
  • Native Oxide and Cleanroom Handling: Bare prime silicon forms a 1–2 nm native oxide in air, necessitating RCA or in-situ cleaning before metallization or epitaxy; strict cleanroom protocols and dry nitrogen storage are required to prevent particulate and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

5-Inch (125.0 ± 0.5 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

10-20 Ω·cm

Thickness

625 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)