| Diameter & Flat: 5-Inch (125.0 ± 0.5 mm) Primary Flat 42.5 mm <110> |
Substrate & Dopant: CZ N-Type / Phosphorus (P) <100>•0.01–0.1 Ω·cm |
Thickness: 625 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+) (~1017–5×1018 cm-3 donor concentration), the wafer combines low substrate series resistance with lower free-carrier IR optical absorption than N++ substrates, supporting vertical diodes, anodic glass bonding, and electrochemical working electrodes.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 5-Inch Dimensional PrecisionStandardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | N-Type / Phosphorus (P) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 0.01–0.1 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 125.0 ± 0.5 mm (5-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 625 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 42.5 ± 2.5 mm | SEMI M1 (125 mm) |
| Secondary Flat | 27.5 ± 2.5 mm secondary flat located 180° ± 5° from primary flat (SEMI M1 125 mm N<100>) | SEMI M1 (125 mm N<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 3 μm•Bow / Warp < 25 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 5-Inch (125 mm), N-Type (100), 0.01-0.1 ohm-cm, 625 um, DSP (This Product) | 5-Inch (125 mm) / DSP | 625 ± 25 μm, N-Type (0.01–0.1 Ω·cm) | SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes |
| 5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, P-Type <100> | Standard SEMI M1 625 μm 125 mm P-type lithography substrate |
| 5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) | 5-Inch (125 mm) / DSP | 625 ± 25 μm, P-Type <100> | Double-side CMP polished 125 mm wafer for IR optics & bonding |
| 5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, N-Type <100> | Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D |
| 5-Inch P-Type <111> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, P-Type <111> | Hexagonal <111> 125 mm lattice for heteroepitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible handling to preserve CMP surface quality and prevent particulate contamination. Environmental exposure must be minimized to avoid native oxide growth and airborne organic contamination.
- Particulate and Surface Contamination Control: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and particle transfer.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring wet processing inside an exhaust fume hood or wet bench when native oxide removal is needed.
- Storage Atmosphere Requirements: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Thermal Processing Compatibility: The 625 ± 25 μm thickness provides flexural rigidity across diffusion tube boats, PECVD/LPCVD cassettes, and vacuum chucks for multi-die fabrication lines.
- Wet Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.
Proper handling preserves mirror-polished CMP cleanliness and ensures reproducible thin-film interfaces across cleanroom processing runs. Sequential solvent cleaning and controlled storage prevent contamination and native oxide interference.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Cleanroom polypropylene cassette, Dry nitrogen cabinet
- Inspect wafer cassette
Verify the cleanroom protective cassette is sealed and undamaged before opening in a controlled environment. - Handle by perimeter edge
Transfer wafers using cleanroom vacuum wands or PTFE/PEEK tweezers while handling strictly by the perimeter edge. - Degrease sequentially
Degrease wafers sequentially in acetone, electronic-grade isopropanol, and DI water followed by N2 blow-drying. - Perform plasma descum
Apply mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols when native oxide removal or RCA standard clean is required. - Store unused wafers properly
Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet.
Why choose 0.01–0.1 Ω·cm N-type silicon instead of a lower-resistivity N++ substrate for vertical devices?
The 0.01–0.1 Ω·cm phosphorus-doped range (~10^17–5×10^18 cm⁻³ donor concentration) balances low substrate series resistance against lower free-carrier IR optical absorption than N++ substrates. This makes it suitable for vertical diodes, anodic glass bonding, and electrochemical working electrodes where excessive doping would degrade infrared transmission. If your process requires minimum series resistance at the expense of IR transparency, a more heavily doped substrate would be the alternative.
Can this 625 μm DSP wafer be used for double-side lithography and anodic or fusion bonding?
Yes. The dual-side CMP mirror finish (DSP, Ra < 0.5 nm) is specified to support double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The SEMI M1 625 ± 25 μm thickness provides the flexural rigidity needed across 125 mm vacuum chucks and bonding fixtures, and the <100> ± 0.5° orientation supports KOH/TMAH anisotropic etching and DRIE when through-features are required.
How should bare prime 5-inch silicon wafers be stored and handled to preserve the CMP surface?
Keep unused wafers sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; the supplied 10 pcs and 25 pcs cassettes immobilize wafer edges to prevent surface contact. Note that bare prime silicon forms a ~1–2 nm native SiO2 film in air, so perform any native-oxide removal or RCA clean inside an exhaust fume hood or wet bench under facility-approved EHS protocols.
The 5-inch prime CZ N-type <100> silicon wafer with 0.01–0.1 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a versatile substrate for MEMS, double-side lithography, and electrochemical prototyping, but its bare surface requires strict cleanroom handling and immediate native-oxide management to preserve interface quality.
Positive
- Low Resistivity N+ Substrate: Phosphorus doping at 0.01–0.1 Ω·cm provides low series resistance for vertical diodes and electrochemical electrodes while maintaining lower free-carrier IR absorption than N++ alternatives.
- Dual-Side CMP Mirror Finish: Double-side polished surfaces with Ra < 0.5 nm enable double-sided lithography, through-wafer IR transmission, and direct fusion or anodic bonding without additional surface preparation.
Trade-offs
- Bare Silicon Native Oxide Growth: Ambient exposure forms a ~1–2 nm native SiO2 layer that must be removed via RCA clean or wet etching before metallization or epitaxy, requiring exhaust fume hood or wet bench facilities.
- Cleanroom Handling and Storage Required: Wafers must be stored in dry nitrogen cabinets and handled only by edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate contamination and preserve CMP surface quality.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.