5-Inch Prime Silicon Wafer P-Type 100-1000 Ω·cm ATOMFAIR®

Price range: $289.00 through $629.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type/Boron silicon wafer, 125.0 ± 0.5 mm, 625 ± 25 μm, 100–1000 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
5-Inch (125.0 ± 0.5 mm)
Primary Flat 42.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•100–1000 Ω·cm
Thickness:
625 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 5-Inch Dimensional Precision

Standardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 125.0 ± 0.5 mm (5.0 Inch)
  • Primary Flat: 42.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 125 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 125.0 ± 0.5 mm (5-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 625 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 42.5 ± 2.5 mm SEMI M1 (125 mm)
Secondary Flat None (SEMI M1 standard for 125 mm P-type <111>) SEMI M1 (125 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 5-Inch (125 mm), P-Type (111), 100-1000 ohm-cm, 625 um, SSP (This Product) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type (100–1000 Ω·cm) SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <100> Standard SEMI M1 625 μm 125 mm P-type lithography substrate
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) 5-Inch (125 mm) / DSP 625 ± 25 μm, P-Type <100> Double-side CMP polished 125 mm wafer for IR optics & bonding
5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, N-Type <100> Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D
5-Inch P-Type <111> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <111> Hexagonal <111> 125 mm lattice for heteroepitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom-compatible storage to prevent particulate contamination and native oxide growth. Handling must avoid surface contact to preserve the CMP mirror finish and sub-nanometer roughness.

  • Cleanroom Storage Environment: Store wafers sealed in the original cleanroom cassette within a dry nitrogen cabinet or desiccator to minimize airborne organic contamination and native oxide growth.
  • Surface Contact Prevention: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching or contaminating the polished front surface.
  • Native Oxide Control: Bare prime silicon forms a 1–2 nm native SiO2 film in ambient air, requiring wet processing inside an exhaust fume hood or wet bench with facility-approved protocols when oxide removal is necessary.
  • Wet Chemical Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.

Proper handling and pre-cleaning procedures preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contaminants prior to deposition or lithography.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system

  1. Inspect wafer cassette
    Verify that the cleanroom cassette is sealed and free of particulate contamination before opening in a controlled environment.
  2. Handle by perimeter edge
    Transfer wafers using a cleanroom vacuum wand or PTFE/PEEK tweezers, contacting only the outer edge to avoid surface damage.
  3. Degrease sequentially
    Immerse wafers in acetone, then electronic-grade isopropanol, then deionized water to remove organic residues.
  4. Dry with nitrogen
    Blow-dry the wafer surface with filtered nitrogen gas until no visible liquid remains.
  5. Perform plasma descum
    Apply a mild oxygen plasma treatment to remove trace organic contaminants prior to photoresist spin coating or PVD/ALD.
  6. Store unused wafers
    Return unused wafers to the original cleanroom cassette and store in a dry nitrogen cabinet to prevent contamination.

Why choose a high-resistivity 100–1000 Ω·cm P-type <111> silicon wafer instead of a standard 1–10 Ω·cm wafer for RF or photodetector work?

The 100–1000 Ω·cm Boron-doped bulk substantially suppresses free-carrier conductive loss and parasitic capacitance compared with standard 1–10 Ω·cm silicon, which is why this substrate is specified for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation. The <111> (± 0.5°) orientation adds hexagonal three-fold surface symmetry and a higher in-plane elastic modulus along key cleavage directions, supporting III-nitride/hexagonal epitaxy such as GaN, AlN, and SiC. If your process instead requires a standard 1–10 Ω·cm <100> lithography substrate, that is a different model in the catalog.

Can this 5-inch P-type <111> SSP wafer be used directly for GaN or AlN epitaxy without an additional buffer or surface treatment?

The dense three-fold <111> lattice is intended to support lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and UHV surface reconstruction studies, but the wafer is supplied bare with no film or coating and carries only a thin ambient native oxide of approximately 1–2 nm. For epitaxy or metallization, the native oxide must be removed using facility-approved wet processing such as an RCA standard clean inside an exhaust fume hood or wet bench. The SSP front surface at Ra < 0.5 nm provides the uniform nucleation surface for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating.

What cleanroom storage and handling is required to preserve the Ra < 0.5 nm CMP surface of this prime 5-inch silicon wafer?

Wafers are supplied in cleanroom protective cassettes (10 pcs or 25 pcs) engineered to immobilize the 5-inch wafer edges and prevent surface contact during transit. Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and keep the surface particle count within the specified ≤ 10 particles per wafer inspection limit.

The 5-inch P-type <111> CZ silicon wafer at 100–1000 Ω·cm combines high bulk resistivity with a densely packed hexagonal lattice, making it a strong substrate choice for RF/microwave loss reduction, III-nitride heteroepitaxy, and UHV surface physics. Its SEMI M1 625 μm geometry and SSP finish (Ra < 0.5 nm) support standard 125 mm cleanroom tooling, though the high resistivity and <111> orientation impose specific process-window and handling constraints.

Positive

  • High-Resistivity RF Substrate: Boron doping at 100–1000 Ω·cm suppresses free-carrier conductive loss and parasitic capacitance, directly benefiting RF/microwave coplanar waveguides, THz/IR optical windows, and photodetector isolation.
  • <111> Lattice for Hexagonal Epitaxy: The <111> ± 0.5° orientation provides three-fold surface symmetry and slower wet alkaline etch kinetics than <100>, supporting GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and UHV surface reconstruction studies.

Trade-offs

  • Native Oxide Requires Wet Processing: Bare prime silicon forms a ~1–2 nm ambient native SiO2 film; removal or RCA cleaning before metallization or epitaxy must be performed in an exhaust fume hood or wet bench under institutional EHS and SDS protocols.
  • Cleanroom Storage and Handling Mandate: Wafers must be stored sealed in a dry nitrogen cabinet or cleanroom desiccator and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

5-Inch (125.0 ± 0.5 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

625 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)