| Diameter & Flat: 5-Inch (125.0 ± 0.5 mm) Primary Flat 42.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•10–20 Ω·cm |
Thickness: 625 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 5-Inch Dimensional PrecisionStandardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 125.0 ± 0.5 mm (5-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 625 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 42.5 ± 2.5 mm | SEMI M1 (125 mm) |
| Secondary Flat | None (SEMI M1 standard for 125 mm P-type <111>) | SEMI M1 (125 mm P<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 5-Inch (125 mm), P-Type (111), 10-20 ohm-cm, 625 um, SSP (This Product) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, P-Type (10–20 Ω·cm) | SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes |
| 5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, P-Type <100> | Standard SEMI M1 625 μm 125 mm P-type lithography substrate |
| 5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) | 5-Inch (125 mm) / DSP | 625 ± 25 μm, P-Type <100> | Double-side CMP polished 125 mm wafer for IR optics & bonding |
| 5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, N-Type <100> | Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D |
| 5-Inch P-Type <111> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, P-Type <111> | Hexagonal <111> 125 mm lattice for heteroepitaxy & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve surface quality. Environmental exposure to particulates, corrosive vapors, and airborne organics degrades the polished CMP surface and compromises thin-film process reproducibility.
- Cleanroom Cassette Storage: Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or desiccator to minimize airborne organic contamination.
- Edge-Only Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to prevent surface contact and particle transfer.
- Native Oxide Awareness: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, which must be removed via RCA clean or wet processing before metallization or epitaxy.
- Wet Processing Safety: Perform all wet-chemical or cleanroom processing strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Proper pre-cleaning and handling of prime silicon wafers preserves the CMP mirror surface and ensures reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum removes organic contamination prior to photoresist spin coating or deposition.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator
- Inspect wafer cassette
Inspect the cleanroom protective cassette for seal integrity and verify that wafers are immobilized without surface contact before opening. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease sequentially
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water to remove organic surface contamination. - Dry with nitrogen
Dry the wafer with a filtered N2 blow-dry to remove residual solvent and water from the polished surface. - Perform plasma descum
Perform a mild O2 plasma descum to remove trace organics prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Remove the native oxide via RCA standard clean or wet processing inside an exhaust fume hood when preparing for metallization or epitaxy. - Store unused wafers
Store unused wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet to prevent recontamination.
Why choose a <111> orientation P-type silicon wafer over <100> for epitaxy or device prototyping?
The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched III-nitride and hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D. It also exhibits a higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics than <100> silicon. This makes it preferable when hexagonal symmetry or etch-rate control is critical, whereas <100> remains the standard for mainstream CMOS lithography.
What is the effect of 10–20 Ω·cm boron doping on C-V characterization and junction capacitance?
Boron doping at 10–20 Ω·cm corresponds to approximately 10^15 cm^-3 dopant density, which minimizes impurity scattering and junction capacitance compared with heavily doped wafers. This moderate resistivity is well suited for MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures where controlled depletion behavior is required. The verified resistivity is measured by four-point probe and documented on the Certificate of Analysis.
How should 5-inch prime silicon wafers be stored and handled to preserve surface quality?
Store wafers sealed inside the original cleanroom protective cassette within a dry nitrogen cabinet or cleanroom desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the Ra < 0.5 nm polished front surface. The cassettes are engineered to immobilize 5-inch wafer edges and prevent surface contact during transit.
This 5-inch prime CZ P-type <111> silicon wafer (10–20 Ω·cm, 625 μm, SSP) is engineered for hexagonal epitaxy, UHV surface physics, and MOS C-V metrology, where its moderate boron doping and three-fold symmetric lattice reduce impurity scattering and support lattice-matched III-nitride growth. Its SEMI M1 geometry and sub-nanometer CMP finish ensure compatibility with 125 mm vacuum chucks and mask aligners, though the bare, uncoated surface requires strict cleanroom handling and immediate native-oxide management before downstream processing.
Positive
- Moderate Resistivity Reduces Scattering: Boron-doped to 10–20 Ω·cm (~10^15 cm⁻³), this substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, directly benefiting MOS C-V gate characterization and minority-carrier diffusion studies.
- <111> Lattice for Hexagonal Epitaxy: The densely packed <111> (± 0.5°) orientation provides three-fold surface symmetry and slower wet alkaline etch kinetics than <100> silicon, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction experiments.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air; native oxide removal or RCA standard clean must be performed in an exhaust fume hood or wet bench using facility-approved protocols before metallization or epitaxy.
- Strict Cleanroom Handling Mandatory: The mirror-polished SSP surface (Ra < 0.5 nm) is vulnerable to particulate and organic contamination; wafers must be handled by the perimeter edge with vacuum wands or PTFE/PEEK tweezers and stored sealed in a dry nitrogen cabinet or cleanroom desiccator.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).