| Diameter & Flat: 5-Inch (125.0 ± 0.5 mm) Primary Flat 42.5 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <111>•1–10 Ω·cm |
Thickness: 625 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: SSP (Ra < 0.5 nm) Polished Front / Fine-Ground Back |
1. Scientific Overview & Substrate Electrical Properties
5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 1–10 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.
Doped with Boron to an industry-standard 1–10 Ω·cm semiconducting resistivity range, the wafer provides a well-characterized majority-hole carrier profile for MOSFET/CMOS device prototyping, Schottky barrier testing, PECVD/ALD dielectric C-V metrology, and general thin-film deposition.
Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.
5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 5-Inch Dimensional PrecisionStandardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 1–10 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <111> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 125.0 ± 0.5 mm (5-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 625 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 42.5 ± 2.5 mm | SEMI M1 (125 mm) |
| Secondary Flat | None (SEMI M1 standard for 125 mm P-type <111>) | SEMI M1 (125 mm P<111>) |
| Surface Polish & Roughness | Single-Side Polished (SSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Total Thickness Variation (TTV) & Bow/Warp | TTV < 5 μm•Bow / Warp < 30 μm | Non-Contact Optical Flatness |
| Surface Particle Inspection | ≤ 10 particles / wafer (Cleanroom Audit) | Bright-Light & Laser Surface Scan |
| Available Pack Sizes | 10 pcs, 25 pcs cleanroom protective cassettes | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
- Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (1–10 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 5-Inch (125 mm), P-Type (111), 1-10 ohm-cm, 625 um, SSP (This Product) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, P-Type (1–10 Ω·cm) | SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes |
| 5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, P-Type <100> | Standard SEMI M1 625 μm 125 mm P-type lithography substrate |
| 5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) | 5-Inch (125 mm) / DSP | 625 ± 25 μm, P-Type <100> | Double-side CMP polished 125 mm wafer for IR optics & bonding |
| 5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) | 5-Inch (125 mm) / SSP | 625 ± 25 μm, N-Type <100> | Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D |
| 4-Inch P-Type <100> Wafer (1–10 Ω·cm, 525 μm SSP) | 4-Inch (100 mm) / SSP | 525 ± 25 μm, P-Type <100> | Compact 100 mm university cleanroom standard substrate |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Prime-grade virgin silicon wafers require cleanroom-compatible storage and edge-only handling to preserve the CMP-polished front surface and prevent particulate contamination. Environmental exposure to airborne organics, corrosive vapors, and moisture must be minimized to maintain sub-nanometer surface roughness and native oxide reproducibility.
- Cleanroom Storage Atmosphere: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
- Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
- Native Oxide Sensitivity: Bare prime silicon forms an ambient approximately 1–2 nm native SiO2 film in air, which must be accounted for prior to metallization or epitaxial processing.
- Wet-Chemical Processing Containment: All wet-chemical or cleanroom processing must be performed strictly inside an exhaust fume hood or wet bench following institutional EHS and SDS safety protocols.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs by following sequential solvent cleaning, plasma descum, and controlled storage procedures. Each step must be executed under institutional EHS and SDS safety protocols.
Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system
- Inspect cassette and wafer
Inspect the cleanroom protective cassette and wafer edges for particulate contamination or physical damage before opening. - Transfer wafer by edge
Transfer the wafer from the cassette using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge. - Degrease sequentially
Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water inside an exhaust fume hood or wet bench. - Dry with nitrogen
Dry the wafer with a nitrogen blow-dry to remove residual solvent and water from the polished surface. - Apply mild O2 plasma descum
Apply a mild O2 plasma descum to the wafer prior to photoresist spin coating or PVD/ALD deposition. - Remove native oxide if required
Remove the ambient approximately 1–2 nm native SiO2 film via RCA standard clean or wet processing inside an exhaust fume hood when metallization or epitaxy requires an oxide-free interface. - Store unused wafers sealed
Store unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Why choose a <111> oriented silicon wafer over <100> for epitaxy or device prototyping?
The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched hexagonal epitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies, whereas <100> is the standard for CMOS lithography. This wafer is specified at <111> ± 0.5° with a 42.5 ± 2.5 mm primary flat along <110> ± 1°, and its higher in-plane elastic modulus along key cleavage directions and slower wet alkaline etch kinetics make it preferable for discrete power/bipolar R&D and III-nitride heteroepitaxy.
Can this 5-inch P-type <111> wafer be used directly in a tube furnace for thermal oxidation without a pre-clean?
Yes, the wafer is a bare prime silicon substrate with no film or coating, carrying only a thin ambient native oxide of approximately 1–2 nm, so it can be loaded directly into a tube furnace for in-house dry/wet thermal SiO2 growth or LPCVD Si3N4. For applications requiring native oxide removal or RCA standard clean before metallization or epitaxy, wet processing must be performed in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.
What are the storage and handling requirements to maintain the Ra < 0.5 nm polished surface of this prime silicon wafer?
Wafers must be stored sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and particulate dust. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, as the single-side polished front surface has a measured roughness of Ra < 0.5 nm and is verified to ≤ 10 particles per wafer by bright-light and laser surface scan.
The 5-inch P-type <111> prime CZ silicon wafer with 1–10 Ω·cm boron doping and SSP finish (Ra < 0.5 nm) is a well-characterized substrate for hexagonal epitaxy, thin-film deposition, and device prototyping, though its <111> orientation and single-side polish impose specific processing constraints.
Positive
- Hexagonal Lattice for Epitaxy: The <111> crystal orientation provides three-fold surface symmetry and slower wet alkaline etch kinetics, supporting lattice-matched GaN/AlN/SiC heteroepitaxy and UHV surface reconstruction studies.
- Sub-Nanometer CMP Surface: Single-side polished front with Ra < 0.5 nm ensures uniform nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating.
Trade-offs
- Single-Side Polish Limits Backside Use: The fine-ground back surface prevents double-side processing such as backside alignment or IR transmission applications that require a polished rear face.
- Native Oxide Requires Removal: Bare prime silicon forms a ~1–2 nm native SiO2 film in air, necessitating wet-chemical or plasma cleaning before metallization or epitaxy to ensure ohmic interfaces.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).