5-Inch Prime CZ Silicon Wafer P-Type 625μm SSP ATOMFAIR®

Price range: $269.00 through $599.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime-grade 5-inch (125 mm) CZ silicon wafer, P-type boron-doped, 100–1000 Ω·cm, orientation, 625 ± 25 μm, SSP Ra < 0.5 nm. In stock.

Diameter & Flat:
5-Inch (125.0 ± 0.5 mm)
Primary Flat 42.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•100–1000 Ω·cm
Thickness:
625 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 100–1000 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Lightly Boron-doped to 100–1000 Ω·cm, this high-resistivity CZ substrate substantially suppresses free-carrier conductive loss and parasitic capacitance, making it well suited for RF/microwave coplanar waveguides, THz/IR optical windows (especially DSP), photodetectors, and MEMS sensor isolation.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 5-Inch Dimensional Precision

Standardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 125.0 ± 0.5 mm (5.0 Inch)
  • Primary Flat: 42.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 27.5 ± 2.5 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 125 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 100–1000 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 125.0 ± 0.5 mm (5-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 625 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 42.5 ± 2.5 mm SEMI M1 (125 mm)
Secondary Flat 27.5 ± 2.5 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 125 mm P<100>) SEMI M1 (125 mm P<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (100–1000 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 5-Inch (125 mm), P-Type (100), 100-1000 ohm-cm, 625 um, SSP (This Product) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type (100–1000 Ω·cm) SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <100> Standard SEMI M1 625 μm 125 mm P-type lithography substrate
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) 5-Inch (125 mm) / DSP 625 ± 25 μm, P-Type <100> Double-side CMP polished 125 mm wafer for IR optics & bonding
5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, N-Type <100> Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D
5-Inch P-Type <111> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <111> Hexagonal <111> 125 mm lattice for heteroepitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin monocrystalline silicon wafers require cleanroom-compatible storage and edge-only handling to preserve the CMP-polished surface. Environmental exposure to particulates, corrosive vapors, and airborne organics must be minimized to prevent surface contamination and native oxide growth.

  • Cleanroom Storage Atmosphere: Store wafers sealed inside the original cleanroom polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Edge-Only Handling Requirement: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contacting the polished front surface.
  • Native Oxide Formation: Bare prime silicon forms an ambient approximately 1–2 nm native SiO2 film in air, which must be removed via RCA standard clean or wet processing before metallization or epitaxy.
  • Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols, with native oxide removal performed inside an exhaust fume hood or wet bench.
  • Surface Contamination Control: Keep unused wafers sealed inside the original cleanroom cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Proper pre-cleaning and handling procedures preserve the mirror-polished CMP surface and ensure reproducible thin-film interfaces. Sequential solvent cleaning followed by plasma descum prepares the wafer for photoresist spin coating or PVD/ALD deposition.

Required Equipment: Cleanroom vacuum wand or PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system, Dry nitrogen cabinet or cleanroom desiccator

  1. Inspect wafer cassette
    Inspect the cleanroom protective cassette for edge immobilization and confirm wafers are seated without surface contact before opening.
  2. Transfer wafer by edge
    Transfer the wafer strictly by its perimeter edge using a cleanroom vacuum wand or PTFE/PEEK tweezers.
  3. Degrease sequentially
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry with nitrogen
    Blow-dry the wafer with N2 until all solvent residue is removed from the polished surface.
  5. Perform plasma descum
    Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition.
  6. Remove native oxide if required
    Perform RCA standard clean or native oxide removal inside an exhaust fume hood or wet bench using facility-approved protocols when metallization or epitaxy requires an oxide-free interface.
  7. Store unused wafers sealed
    Return unused wafers to the original cleanroom polypropylene cassette box and store within a dry nitrogen cabinet.

Why does this 5-inch silicon wafer specify 100–1000 Ω·cm resistivity instead of the standard 1–10 Ω·cm?

The 100–1000 Ω·cm Boron-doped specification is a high-resistivity grade chosen to suppress free-carrier conductive loss and parasitic capacitance, which is critical for RF/microwave coplanar waveguides, THz/IR optical windows, photodetectors, and MEMS sensor isolation. Standard 1–10 Ω·cm P-type wafers are optimized for lithography and CMOS prototyping, whereas this lightly doped substrate trades lower carrier concentration for reduced dielectric loss. The trade-off is that highly resistive silicon is not intended as a low-resistance device layer or ohmic contact substrate.

Can this <100> P-type SSP wafer be used for KOH or TMAH anisotropic wet etching and DRIE?

Yes. The wafer is sliced along the <100> (± 0.5°) plane, which supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and Bosch deep reactive ion etching (DRIE) for MEMS micromachining. The cubic <100> surface also provides four-fold rotational symmetry with clean perpendicular cleaving along <110> planes. Note that the backside is fine-ground rather than polished, so backside lithography or bonding should account for that surface finish.

What handling and storage conditions are required to preserve the SSP Ra < 0.5 nm surface before thin-film deposition?

Wafers must be handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and unused wafers should remain sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors. Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, so if native oxide removal or RCA cleaning is required before metallization or epitaxy, perform wet processing only in an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols. Pre-cleaning typically follows sequential acetone, electronic-grade IPA, and DI water degreasing with N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.

The 5-inch prime CZ P-type <100> silicon wafer with 100–1000 Ω·cm resistivity and SSP finish offers a high-resistivity, low-loss substrate ideal for RF/microwave and MEMS applications, but its bare surface and tight flatness tolerances demand strict cleanroom handling and immediate native-oxide management.

Positive

  • High-Resistivity Substrate: Boron-doped to 100–1000 Ω·cm, this wafer suppresses free-carrier conductive loss and parasitic capacitance, making it suitable for RF/microwave coplanar waveguides, THz/IR optical windows, and photodetectors.
  • Precision <100> Orientation: The <100> ± 0.5° crystal orientation provides four-fold rotational symmetry, clean perpendicular cleaving along <110> planes, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions for MEMS micromachining.

Trade-offs

  • Native Oxide Formation: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, requiring wet-chemical removal (e.g., RCA clean) before metallization or epitaxy, which must be performed in an exhaust fume hood or wet bench following institutional EHS protocols.
  • Cleanroom Handling Required: To preserve the mirror-polished CMP surface (Ra < 0.5 nm) and maintain ≤10 particles per wafer, wafers must be stored in a dry nitrogen cabinet and handled strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

5-Inch (125.0 ± 0.5 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

100-1000 Ω·cm

Thickness

625 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)