5-Inch Prime Silicon Wafer P-Type 10-20 Ω·cm ATOMFAIR®

Price range: $249.00 through $529.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type 5-inch (125 mm) silicon wafer, 10–20 Ω·cm, 625 ± 25 μm, SSP Ra < 0.5 nm. SEMI M1 flats. In stock.

Diameter & Flat:
5-Inch (125.0 ± 0.5 mm)
Primary Flat 42.5 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<100>•10–20 Ω·cm
Thickness:
625 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

5-Inch (125 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 125.0 ± 0.5 mm diameter and 625 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.

Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.

5-Inch (125 mm) Thickness & Process Compatibility Note: The SEMI M1 standard 625 ± 25 μm mechanical thickness provides high flexural rigidity across 125 mm stepper/aligner vacuum chucks, diffusion tube boats, PECVD/LPCVD cassettes, and multi-die fabrication lines. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)

SEMI M1 5-Inch Dimensional Precision

Standardized 125.0 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 125.0 ± 0.5 mm (5.0 Inch)
  • Primary Flat: 42.5 ± 2.5 mm along <110> ± 1°
  • Secondary Flat: 27.5 ± 2.5 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 125 mm P<100>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 10–20 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <100> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 125.0 ± 0.5 mm (5-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 625 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 42.5 ± 2.5 mm SEMI M1 (125 mm)
Secondary Flat 27.5 ± 2.5 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 125 mm P<100>) SEMI M1 (125 mm P<100>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Total Thickness Variation (TTV) & Bow/Warp TTV < 5 μm•Bow / Warp < 30 μm Non-Contact Optical Flatness
Surface Particle Inspection ≤ 10 particles / wafer (Cleanroom Audit) Bright-Light & Laser Surface Scan
Available Pack Sizes 10 pcs, 25 pcs cleanroom protective cassettes Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications

  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.

Packaging, Storage & Handling Protocol

Wafers are supplied in cleanroom protective cassettes (10 pcs, 25 pcs options) engineered to immobilize 5-inch wafer edges and prevent surface contact during international transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters, thicknesses, and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 5-Inch (125 mm), P-Type (100), 10-20 ohm-cm, 625 um, SSP (This Product) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type (10–20 Ω·cm) SEMI M1 625 μm 125 mm wafer in 10 pcs / 25 pcs cassettes
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <100> Standard SEMI M1 625 μm 125 mm P-type lithography substrate
5-Inch P-Type <100> Wafer (1–10 Ω·cm, 625 μm DSP) 5-Inch (125 mm) / DSP 625 ± 25 μm, P-Type <100> Double-side CMP polished 125 mm wafer for IR optics & bonding
5-Inch N-Type <100> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, N-Type <100> Phosphorus-doped 125 mm N-type wafer for power & CMOS R&D
5-Inch P-Type <111> Wafer (1–10 Ω·cm, 625 μm SSP) 5-Inch (125 mm) / SSP 625 ± 25 μm, P-Type <111> Hexagonal <111> 125 mm lattice for heteroepitaxy & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 5-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original cleanroom polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require particulate-controlled storage and edge-only contact to preserve the CMP mirror surface. Ambient native oxide growth and airborne organic contamination must be managed prior to lithography or thin-film processing.

  • Particulate and Vapor Exposure: Store wafers sealed in the original cleanroom cassette inside a dry nitrogen cabinet or desiccator away from particulate dust and corrosive vapors.
  • Surface Contact Restriction: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid scratching the polished front surface.
  • Native Oxide Formation: Bare prime silicon develops an ambient native SiO2 film of approximately 1–2 nm in air, which must be removed before metallization or epitaxy if an oxide-free interface is required.
  • Wet-Chemical Processing Environment: Perform RCA standard cleans, native oxide removal, or other wet processing strictly inside an exhaust fume hood or wet bench under facility-approved EHS and SDS protocols.
  • Cassette Immobilization: Keep unused wafers immobilized in the cleanroom polypropylene cassette to prevent edge chipping and surface-to-surface contact during storage.

Proper handling preserves the sub-nanometer CMP finish and prevents contamination that degrades thin-film nucleation and lithographic resolution. Sequential solvent cleaning and edge-only manipulation are required before any deposition or patterning step.

Required Equipment: Cleanroom vacuum wand, PTFE or PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, Exhaust fume hood or wet bench

  1. Inspect cassette and wafer
    Inspect the cleanroom cassette and wafer edges for particulate contamination or chipping before removing the wafer.
  2. Extract wafer by edge
    Extract the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers applied only to the perimeter edge.
  3. Degrease in solvent sequence
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry and descum
    Blow-dry the wafer with N2 and apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  5. Remove native oxide if required
    Perform RCA standard clean or native oxide removal inside an exhaust fume hood or wet bench when an oxide-free interface is required before metallization or epitaxy.
  6. Return unused wafers to storage
    Return unused wafers to the original cleanroom cassette and store sealed inside a dry nitrogen cabinet.

What is the difference between 10–20 Ω·cm and 1–10 Ω·cm boron-doped silicon wafers for MOS C-V characterization?

The 10–20 Ω·cm resistivity of this wafer corresponds to a lower boron dopant density (~10^15 cm⁻³) than 1–10 Ω·cm substrates, which reduces impurity scattering and junction capacitance. This makes it preferable for MOS C-V gate characterization and minority-carrier diffusion studies where a lightly doped depletion region is required. If your process needs higher bulk conductivity for ohmic contact formation or power device prototyping, a 1–10 Ω·cm wafer is the more appropriate choice.

Can this 5-inch SSP wafer be used for KOH anisotropic etching and DRIE MEMS micromachining?

Yes. The <100> (± 0.5°) crystal orientation supports predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions and is compatible with Bosch deep reactive ion etching (DRIE). The fine-ground back surface provides handling robustness, while the SSP front surface (Ra < 0.5 nm) is suitable for subsequent lithographic patterning. Note that the backside is not polished, so backside alignment or double-sided processing would require a DSP variant.

How should bare prime silicon wafers be stored and handled to preserve the CMP surface before thermal oxidation?

Store wafers sealed in the original cleanroom polypropylene cassette inside a dry nitrogen cabinet or desiccator, away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid contaminating the Ra < 0.5 nm polished front surface. Bare prime silicon carries only a ~1–2 nm native oxide, so perform any RCA clean or native oxide removal immediately before thermal oxidation or metallization inside an exhaust fume hood following institutional EHS protocols.

The 5-inch prime CZ P-type <100> silicon wafer at 10–20 Ω·cm and 625 μm thickness offers a balanced substrate for MOS C-V characterization, anisotropic KOH/TMAH micromachining, and thin-film nucleation, with SEMI M1 flats and sub-nanometer SSP finish ensuring tooling compatibility. Its bare, uncoated surface and moderate resistivity require cleanroom handling and pre-clean protocols to manage the native oxide and preserve interface quality.

Positive

  • Moderate resistivity reduces junction capacitance: Boron doping at 10–20 Ω·cm minimizes impurity scattering and junction capacitance compared to heavily doped wafers, supporting MOS C-V gate characterization and minority-carrier diffusion studies.
  • CMP mirror surface enables uniform thin films: Single-side polished front with Ra < 0.5 nm provides reproducible nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating.

Trade-offs

  • Native oxide requires removal before metallization: Bare prime silicon forms a 1–2 nm ambient native SiO2 film in air; wet processing or RCA clean must be performed in an exhaust fume hood or wet bench to ensure ohmic interfaces.
  • Cleanroom handling mandatory to prevent contamination: Wafers must be stored in dry nitrogen cabinets and handled by perimeter edge with vacuum wands or PTFE/PEEK tweezers to avoid particulate and organic contamination.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

10 pcs, 25 pcs

Diameter

5-Inch (125.0 ± 0.5 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

10-20 Ω·cm

Thickness

625 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)