3-Inch P-Type Silicon Wafer 0.001-0.005 Ω·cm ATOMFAIR®

$299.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ P-Type silicon wafer, 76.2 ± 0.25 mm, 380 ± 25 μm, 0.001–0.005 Ω·cm, SSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. In stock.

Diameter & Flat:
3-Inch (76.2 ± 0.25 mm)
Primary Flat 22.22 mm <110>
Substrate & Dopant:
CZ P-Type / Boron (B)
<111>•0.001–0.005 Ω·cm
Thickness:
380 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
SSP (Ra < 0.5 nm)
Polished Front / Fine-Ground Back

1. Scientific Overview & Substrate Electrical Properties

3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 0.001–0.005 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features a mirror-polished front surface (CMP, Ra < 0.5 nm) and fine-ground back surface.

Degenerately Boron-doped to 0.001–0.005 Ω·cm (P++) (~1019–1020 cm-3 carrier concentration), the wafer provides metallic-like bulk conductivity suitable for low-resistance ohmic contacts, cryogenic back-gated 2D FETs, electrochemical electrodes, and high-power epitaxy.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Single-Side Polished (SSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 3-Inch Dimensional Precision

Standardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 76.2 ± 0.25 mm (3.0 Inch)
  • Primary Flat: 22.22 ± 3.17 mm along <110> ± 1°
  • Secondary Flat: None (SEMI M1 standard for 76.2 mm P-type <111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant P-Type / Boron (B) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.001–0.005 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 76.2 ± 0.25 mm (3-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 380 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 22.22 ± 3.17 mm SEMI M1 (76.2 mm)
Secondary Flat None (SEMI M1 standard for 76.2 mm P-type <111>) SEMI M1 (76.2 mm P<111>)
Surface Polish & Roughness Single-Side Polished (SSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Thin-Film Deposition & Photolithography: Mirror-polished front surface (SSP, Ra < 0.5 nm) ensures uniform nucleation for PVD sputtering, ALD, e-beam evaporation, and high-resolution photoresist spin coating;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (0.001–0.005 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 3-Inch (76.2 mm), P-Type (111), 0.001-0.005 ohm-cm, 380 um, SSP (This Product) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type (0.001–0.005 Ω·cm) SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools
3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <100> Standard 76.2 mm P<100> bare lithography substrate
3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 3-Inch (76.2 mm) / DSP 380 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & wafer bonding
3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, N-Type <100> Phosphorus-doped N<100> substrate for Schottky & diode R&D
3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 3-Inch (76.2 mm) / SSP 380 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Bare prime silicon forms a native oxide layer in ambient air, requiring controlled atmosphere storage to prevent organic contamination. The mirror-polished surface is sensitive to particulate and chemical exposure, necessitating cleanroom handling protocols.

  • Native Oxide Formation: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, which must be removed before metallization or epitaxy.
  • Storage Atmosphere: Store wafers sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Surface Contamination Risk: Airborne organic contamination can degrade the mirror-polished CMP surface, affecting thin-film nucleation and lithography reproducibility.
  • Handling Contact Restrictions: Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface damage.

Proper handling preserves the mirror-polished surface and prevents contamination during cleanroom processing. Sequential solvent cleaning and plasma descum are required before photoresist spin coating or thin-film deposition.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench, O2 plasma descum system

  1. Inspect wafer cassette
    Inspect the sealed 25-wafer cleanroom cassette for integrity before opening in a controlled environment.
  2. Transfer wafer
    Transfer the wafer using a cleanroom vacuum wand or PTFE/PEEK tweezers, handling only by the perimeter edge.
  3. Degrease wafer
    Degrease the wafer sequentially in acetone, electronic-grade isopropanol, and DI water.
  4. Dry wafer
    Dry the wafer with nitrogen blow-drying to remove residual solvents.
  5. Perform plasma descum
    Perform a mild O2 plasma descum to remove organic contaminants prior to photoresist spin coating or PVD/ALD.
  6. Remove native oxide
    Remove native oxide via wet processing inside an exhaust fume hood or wet bench using facility-approved protocols when required before metallization or epitaxy.
  7. Store unused wafers
    Store unused wafers sealed inside the original polypropylene cassette within a dry nitrogen cabinet to minimize airborne organic contamination.

Why choose a <111> orientation P++ silicon wafer over standard <100> for epitaxy or device prototyping?

The <111> orientation provides a densely packed three-fold surface symmetry that supports lattice-matched III-nitride heteroepitaxy (GaN, AlN, SiC) and UHV surface reconstruction studies, while its slower wet alkaline etch kinetics enable more controlled anisotropic etching than <100> silicon. Combined with degenerate boron doping at 0.001–0.005 Ω·cm (P++), this substrate delivers metallic-like bulk conductivity for low-resistance ohmic contacts and cryogenic back-gated 2D FETs. However, <111> wafers are not a drop-in replacement for <100> in standard CMOS lines, where <100> remains the industry baseline.

Can this 3-inch P++ <111> wafer be used directly in a tube furnace for thermal oxidation without a pre-clean?

Yes, the wafer is a bare prime silicon substrate with only a thin ambient native oxide (~1–2 nm), so it can be loaded directly into a tube furnace for in-house dry/wet thermal SiO2 growth. For reproducible interfaces, however, the source recommends solvent pre-cleaning (acetone, IPA, DI water) followed by N2 blow-drying and mild O2 plasma descum before oxidation or epitaxy. If native oxide removal or RCA clean is required, perform wet processing strictly in an exhaust fume hood or wet bench following institutional EHS and SDS protocols.

What handling and storage practices are required to maintain the Ra < 0.5 nm polished surface of this SSP wafer?

Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and keep unused wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator. This prevents particulate dust, airborne organic contamination, and corrosive vapors from degrading the CMP mirror finish (Ra < 0.5 nm). The fine-ground back surface is not designed for device processing and should not be used as a reference for lithography alignment.

The 3-inch P++ <111> CZ silicon wafer combines degenerate boron doping (0.001–0.005 Ω·cm) with a CMP-polished front surface (Ra < 0.5 nm) for low-resistance ohmic contacts and hexagonal epitaxy, but its <111> orientation and single-side polish impose constraints on backside processing and etch kinetics relative to <100> alternatives.

Positive

  • Degenerate P++ doping for ohmic contacts: Boron doping at 0.001–0.005 Ω·cm (~10^19–10^20 cm^-3) provides metallic-like bulk conductivity, enabling low-resistance ohmic contacts and cryogenic back-gated 2D FET operation without additional implant steps.
  • CMP front surface for epitaxy and lithography: Single-side CMP polishing achieves Ra < 0.5 nm on the front face, supporting uniform nucleation for PVD, ALD, e-beam evaporation, and high-resolution photoresist spin coating in thin-film and device prototyping.

Trade-offs

  • Single-side polish limits backside processing: The fine-ground back surface (SSP configuration) is not mirror-polished, restricting use in double-side lithography, wafer bonding, or backside alignment processes that require DSP substrates.
  • Native oxide and wet-bench dependency: Bare prime silicon forms a 1–2 nm ambient native SiO2 film, requiring RCA clean or native-oxide removal in an exhaust fume hood or wet bench under institutional EHS protocols before metallization or epitaxy.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

3-Inch (76.2 ± 0.25 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

P-Type / Boron (B)

Orientation

± 0.5°

Resistivity

0.001-0.005 Ω·cm

Thickness

380 ± 25 μm

Surface Finish

Single-Side Polished (SSP, Ra < 0.5 nm)