| Diameter & Flat: 3-Inch (76.2 ± 0.25 mm) Primary Flat 22.22 mm <110> |
Substrate & Dopant: CZ P-Type / Boron (B) <100>•10–20 Ω·cm |
Thickness: 380 ± 25 μm Prime-Grade Virgin Wafer |
Surface Polish: DSP (Ra < 0.5 nm) Dual-Side Mirror-Polished (CMP) |
1. Scientific Overview & Substrate Electrical Properties
3-Inch (76.2 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Boron-doped to a verified resistivity of 10–20 Ω·cm along the <100> (± 0.5°) crystal orientation. Manufactured to a 76.2 ± 0.25 mm diameter and 380 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).
Boron-doped to 10–20 Ω·cm (~1015 cm-3 dopant density), this moderate-resistivity substrate minimizes impurity scattering and junction capacitance compared with heavily doped wafers, supporting MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures.
Sliced along the industry-standard <100> (± 0.5°) plane, the cubic surface exhibits four-fold rotational symmetry with clean perpendicular cleaving along <110> planes, low Si/SiO2 interface state density, and predictable anisotropic wet-etch V-groove formation in KOH/TMAH solutions.
3-Inch Chamber Compatibility & Surface State Note: The 3-inch (76.2 mm) format delivers ~2.25× the usable patterning area of a 2-inch wafer while fitting standard 3-inch mask aligners, PECVD/ALD platens, tube/RTA furnaces, and multi-die sputtering chucks. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.
2. Wafer Geometry & Batch Verification Standards
CMP Surface Roughness ControlChemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.
|
SEMI M1 3-Inch Dimensional PrecisionStandardized 76.2 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.
|
3. Verified Inspection Specifications
All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):
| Parameter | Inspection Specification | Measurement / Standard Basis |
|---|---|---|
| Wafer Grade | Prime Grade (Virgin monocrystalline substrate) | Factory Lot Traceability |
| Crystal Growth Method | CZ (Czochralski) monocrystalline silicon | Ingot Boule Record |
| Conductivity Type & Dopant | P-Type / Boron (B) | Hot-Probe / Bulk Doping Spec |
| Electrical Resistivity | 10–20 Ω·cm | Four-Point Probe (4PP) |
| Crystal Orientation | <100> (± 0.5°) | X-Ray Diffraction (XRD) |
| Diameter & Tolerance | 76.2 ± 0.25 mm (3-Inch) | SEMI M1 / Optical Gauge |
| Substrate Thickness | 380 ± 25 μm | SEMI M1 / Capacitance Gauge |
| Primary Orientation Flat | Location: <110> ± 1°•Length: 22.22 ± 3.17 mm | SEMI M1 (76.2 mm) |
| Secondary Flat | 11.18 ± 1.52 mm secondary flat located 90° ± 5° clockwise from primary flat (SEMI M1 76.2 mm P<100>) | SEMI M1 (76.2 mm P<100>) |
| Surface Polish & Roughness | Double-Side Polished (DSP)•Ra < 0.5 nm | CMP Finish / AFM Audit |
| Film / Coating | None (Bare Prime Silicon) | Visual & Cleanroom Inspection |
| Pack Size (MOQ) | 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) | Cleanroom Cassette Packaging |
4. Target Applications, Packaging & Cleanroom Handling
Primary Research & Fabrication Applications
- Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
- MEMS & Anisotropic Silicon Micromachining: Cleanroom <100> crystal plane supports KOH / TMAH wet anisotropic etching and Bosch deep reactive ion etching (DRIE);
- Semiconductor Device & Electrode Prototyping: Controlled Boron-doped (10–20 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
- In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol
Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 3-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
Quality Standards & Batch Verification
Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.
5. Related Silicon Wafers & Substrates Selection Matrix
Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:
| Product Model | Diameter / Finish | Thickness / Conductivity | Key Differentiator & Use Case |
|---|---|---|---|
| Prime Silicon Wafer, 3-Inch (76.2 mm), P-Type (100), 10-20 ohm-cm, 380 um, DSP (This Product) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type (10–20 Ω·cm) | SEMI M1 380 μm thickness, 25 pcs cassette for 3-inch R&D tools |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <100> | Standard 76.2 mm P<100> bare lithography substrate |
| 3-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) | 3-Inch (76.2 mm) / DSP | 380 ± 25 μm, P-Type <100> | Double-side CMP polished for IR optics & wafer bonding |
| 3-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, N-Type <100> | Phosphorus-doped N<100> substrate for Schottky & diode R&D |
| 3-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) | 3-Inch (76.2 mm) / SSP | 380 ± 25 μm, P-Type <111> | Hexagonal <111> lattice for III-nitride & UHV growth |
Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub | Need custom dicing or thicknesses? Inquire About Custom Wafer Services
6. Cleanroom Handling & Surface Preparation Guidelines
To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:
- Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
- Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
- Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.
Custom Wafer Dicing, Lapping & Thermal Oxidation Services
Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).
Bare prime silicon wafers carry a thin ambient native oxide and are sensitive to particulate contamination, airborne organics, and corrosive vapors. Storage and handling must preserve the CMP mirror finish and prevent surface contact.
- Native Oxide Formation: Bare prime silicon forms an ambient 1–2 nm native SiO2 film in air, requiring controlled removal before metallization or epitaxy.
- Particulate and Organic Contamination: Unsealed wafers are susceptible to airborne particulate dust and organic contamination that degrade lithography and thin-film interfaces.
- Corrosive Vapor Exposure: Storage near corrosive vapors must be avoided to prevent surface degradation of the CMP-polished finish.
- Edge-Contact Restriction: Direct surface contact must be avoided; wafers require perimeter-edge handling with cleanroom vacuum wands or PTFE/PEEK tweezers.
- Wet-Chemical Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols inside an exhaust fume hood or wet bench.
Preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs. Follow sequential solvent cleaning, plasma descum, and controlled storage procedures.
Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Dry nitrogen cabinet or cleanroom desiccator, O2 plasma descum system
- Inspect Cassette and Wafer Edges
Inspect the 25-wafer cleanroom cassette and wafer edges for particulate contamination or physical damage before opening. - Handle by Perimeter Edge
Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface contact. - Degrease Sequentially
Degrease diced dies or whole 3-inch wafers sequentially in acetone, electronic-grade isopropanol, and DI water. - Blow-Dry with Nitrogen
Blow-dry the wafer surface with N2 to remove residual solvent and water before further processing. - Apply Mild O2 Plasma Descum
Apply a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD deposition. - Remove Native Oxide Under Exhaust
Perform native oxide removal or RCA standard clean strictly inside an exhaust fume hood or wet bench using facility-approved protocols. - Store in Sealed Cassette
Store unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet.
What is the resistivity and dopant specification of this 3-inch silicon wafer, and how does it affect MOS C-V characterization?
This wafer is P-Type, Boron-doped with a bulk resistivity of 10–20 Ω·cm, corresponding to approximately 10^15 cm^-3 dopant density. This moderate resistivity minimizes impurity scattering and junction capacitance compared with heavily doped wafers, making it suitable for MOS C-V gate characterization, minority-carrier diffusion studies, and photodiode test structures. Resistivity is verified per batch by four-point probe (4PP) and documented on the Certificate of Analysis.
Can this 3-inch DSP wafer be used for double-side lithography and wafer bonding?
Yes. The wafer is double-side polished (DSP) via CMP with a measured surface roughness of Ra < 0.5 nm on both faces, supporting double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion or anodic bonding. The 76.2 ± 0.25 mm diameter and SEMI M1 flats ensure accurate registration on vacuum chucks and mask aligners. No film or coating is present (bare prime silicon), so users must perform their own pre-bonding clean.
How should these prime silicon wafers be stored and handled to preserve the CMP surface?
Wafers are supplied in a standard 25-wafer cleanroom cassette (25BX) that immobilizes edges and prevents surface contact. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers; bare prime silicon carries only a ~1–2 nm native oxide, so any wet processing must follow institutional EHS and SDS protocols.
The 3-inch prime CZ P-type <100> silicon wafer with 10–20 Ω·cm resistivity and dual-side CMP finish (Ra < 0.5 nm) is a versatile substrate for MEMS, double-side lithography, and in-house oxidation, but its bare surface requires immediate native-oxide control and strict cleanroom handling to preserve interface quality.
Positive
- Dual-Side CMP Enables Bonding: Double-side mirror-polished surfaces (Ra < 0.5 nm) support direct fusion and anodic wafer bonding, double-sided MEMS patterning, and through-wafer IR transmission without additional surface preparation.
- Moderate Resistivity for Device Prototyping: Boron-doped 10–20 Ω·cm resistivity minimizes impurity scattering and junction capacitance, making it suitable for MOS C-V characterization, minority-carrier diffusion studies, and photodiode test structures.
Trade-offs
- Native Oxide Requires Removal: Bare prime silicon forms a 1–2 nm ambient native SiO2 film in air; wet-chemical removal or RCA clean must be performed in an exhaust fume hood or wet bench following institutional EHS protocols before metallization or epitaxy.
- Strict Cleanroom Handling Mandatory: To preserve CMP surface quality, wafers must be stored in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid particulate and organic contamination.
Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.
To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.
Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).