2-Inch N-Type Silicon Wafer 0.01-0.1 Ω·cm DSP ATOMFAIR®

$359.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Prime CZ N-Type silicon wafer, 50.8 mm, 275 μm, 0.01–0.1 Ω·cm, DSP Ra < 0.5 nm. SEMI M1 flats, 25 pcs cassette. Order now.

Diameter & Flat:
2-Inch (50.8 ± 0.2 mm)
Primary Flat 15.88 mm <110>
Substrate & Dopant:
CZ N-Type / Phosphorus (P)
<111>•0.01–0.1 Ω·cm
Thickness:
275 ± 25 μm
Prime-Grade Virgin Wafer
Surface Polish:
DSP (Ra < 0.5 nm)
Dual-Side Mirror-Polished (CMP)

1. Scientific Overview & Substrate Electrical Properties

2-Inch (50.8 mm) Prime CZ Monocrystalline Silicon Wafers are grown via the Czochralski (CZ) process and Phosphorus-doped to a verified resistivity of 0.01–0.1 Ω·cm along the <111> (± 0.5°) crystal orientation. Manufactured to a 50.8 ± 0.2 mm diameter and 275 ± 25 μm thickness, each virgin substrate features dual-side mirror-polished surfaces (CMP, Ra < 0.5 nm).

Phosphorus-doped to a low-resistivity range of 0.01–0.1 Ω·cm (N+), the wafer combines low substrate contact resistance with lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.

Oriented along the densely packed <111> (± 0.5°) crystal plane, the substrate exhibits hexagonal three-fold surface symmetry, higher in-plane elastic modulus along key cleavage directions, and slower wet alkaline etch kinetics than <100> silicon, supporting III-nitride/hexagonal epitaxy (GaN, AlN, SiC), UHV surface reconstruction studies, and discrete power/bipolar R&D.

2-Inch Chamber Compatibility & Surface State Note: The compact 2-inch (50.8 mm) footprint fits research-scale tube furnaces, compact ALD/PECVD chambers, R&D spin coaters, and 2-inch sputtering sample holders without dicing waste. Bare prime silicon carries only a thin ambient native oxide (~1–2 nm), allowing direct in-house thermal oxidation, wet etching, or epitaxial/thin-film growth.

2. Wafer Geometry & Batch Verification Standards

CMP Surface Roughness Control

Chemo-mechanical polishing (CMP) produces a defect-screened mirror surface with sub-nanometer microroughness (Ra < 0.5 nm) for reproducible thin-film growth and lithography.

  • Surface Polish: Double-Side Polished (DSP)
  • Measured Roughness: Ra < 0.5 nm
  • Surface Coating: None (Bare Prime Silicon)
SEMI M1 2-Inch Dimensional Precision

Standardized 50.8 mm diameter and SEMI M1 crystal alignment flats ensure accurate registration on vacuum chucks, mask aligners, and cleanroom cassettes.

  • Diameter: 50.8 ± 0.2 mm (2.0 Inch)
  • Primary Flat: 15.88 ± 1.65 mm along <110> ± 1°
  • Secondary Flat: Located 45° ± 5° clockwise from primary flat (SEMI M1 50.8 mm N<111>)

3. Verified Inspection Specifications

All technical specifications and tolerances below are verified per production batch and documented on the accompanying Certificate of Analysis (CoA):

Parameter Inspection Specification Measurement / Standard Basis
Wafer Grade Prime Grade (Virgin monocrystalline substrate) Factory Lot Traceability
Crystal Growth Method CZ (Czochralski) monocrystalline silicon Ingot Boule Record
Conductivity Type & Dopant N-Type / Phosphorus (P) Hot-Probe / Bulk Doping Spec
Electrical Resistivity 0.01–0.1 Ω·cm Four-Point Probe (4PP)
Crystal Orientation <111> (± 0.5°) X-Ray Diffraction (XRD)
Diameter & Tolerance 50.8 ± 0.2 mm (2-Inch) SEMI M1 / Optical Gauge
Substrate Thickness 275 ± 25 μm SEMI M1 / Capacitance Gauge
Primary Orientation Flat Location: <110> ± 1°•Length: 15.88 ± 1.65 mm SEMI M1 (50.8 mm)
Secondary Flat Located 45° ± 5° clockwise from primary flat (SEMI M1 50.8 mm N<111>) SEMI M1 (50.8 mm N<111>)
Surface Polish & Roughness Double-Side Polished (DSP)•Ra < 0.5 nm CMP Finish / AFM Audit
Film / Coating None (Bare Prime Silicon) Visual & Cleanroom Inspection
Pack Size (MOQ) 25 pcs (1 × 25-wafer cleanroom cassette, 25BX) Cleanroom Cassette Packaging

4. Target Applications, Packaging & Cleanroom Handling

Primary Research & Fabrication Applications
  • Double-Side Lithography, IR Optics & Wafer Bonding: Dual-side CMP finish (DSP, Ra < 0.5 nm) supports double-sided MEMS patterning, through-wafer infrared transmission, and direct fusion/anodic bonding;
  • Hexagonal Epitaxy & UHV Surface Physics: Dense three-fold <111> crystal lattice supports lattice-matched GaN/AlN/SiC heteroepitaxy, graphene/TMDC template growth, and discrete bipolar/power prototyping;
  • Semiconductor Device & Electrode Prototyping: Controlled Phosphorus-doped (0.01–0.1 Ω·cm) base for ohmic contacts, Schottky diodes, electrochemical sensors, and C-V metrology;
  • In-House Oxidation & Material Calibration: Virgin prime wafer for custom tube-furnace dry/wet thermal SiO2 growth, LPCVD Si3N4, and ellipsometry/XRR calibration.
Packaging, Storage & Handling Protocol

Wafers are supplied in a standard 25-wafer protective cleanroom cassette (25 pcs pack, 25BX) engineered to immobilize 2-inch wafer edges and prevent surface contact during transit. Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.

Quality Standards & Batch Verification

Every wafer supplied is strictly a prime-grade, virgin silicon substrate (never test-grade, dummy, or reclaimed wafers). Shipments include a lot-specific Certificate of Analysis (CoA) documenting bulk resistivity, thickness tolerance, crystal orientation, and cleanroom surface inspection criteria.

5. Related Silicon Wafers & Substrates Selection Matrix

Compare standard research diameters and wafer grades in the Silicon Wafers & Substrates catalog:

Product Model Diameter / Finish Thickness / Conductivity Key Differentiator & Use Case
Prime Silicon Wafer, 2-Inch (50.8 mm), N-Type (111), 0.01-0.1 ohm-cm, 275 um, DSP (This Product) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, N-Type (0.01–0.1 Ω·cm) SEMI M1 275 μm thickness, 25 pcs cassette for 2-inch R&D chambers
2-Inch P-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <100> Standard 50.8 mm P<100> bare lithography substrate
2-Inch P-Type <100> Wafer (1–10 Ω·cm DSP) 2-Inch (50.8 mm) / DSP 275 ± 25 μm, P-Type <100> Double-side CMP polished for IR optics & bonding
2-Inch N-Type <100> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, N-Type <100> Phosphorus-doped N<100> wafer for Schottky & diode R&D
2-Inch P-Type <111> Wafer (1–10 Ω·cm SSP) 2-Inch (50.8 mm) / SSP 275 ± 25 μm, P-Type <111> Hexagonal <111> lattice for III-nitride & UHV growth

Browse all research wafers & substrates: Complete Silicon Wafers & Substrates Hub  |  Need custom dicing or thicknesses? Inquire About Custom Wafer Services

6. Cleanroom Handling & Surface Preparation Guidelines

To preserve mirror-polished CMP cleanliness and reproducible thin-film interfaces across cleanroom processing runs:

  • Solvent & Plasma Pre-Cleaning: Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water, followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD;
  • Native Oxide & Ohmic Interface Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air. Where native oxide removal or RCA standard clean is required before metallization or epitaxy, perform wet processing strictly inside an exhaust fume hood or wet bench using facility-approved protocols. Note: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols;
  • Cleanroom Cassette Storage: Keep unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet to minimize airborne organic contamination.

Custom Wafer Dicing, Lapping & Thermal Oxidation Services

Specialized semiconductor substrate engineering and cleanroom processing are available on request. We support custom bulk resistivities, double-side polishing (DSP), custom thermal oxide or LPCVD nitride coatings, custom diameters, and precision diamond-saw dicing (3 × 3 mm, 5 × 5 mm, 10 × 10 mm, and 15 × 15 mm dies).

TAILORED SOLUTIONS FOR UNIVERSITY & INSTITUTIONAL R&D
Official Formal Quotations, University Purchase Orders (POs), Net-Terms for Qualified Academic Laboratories, and Batch Academic Shipments Available.

Prime-grade virgin silicon wafers require cleanroom handling to preserve CMP surface quality and prevent particulate contamination. Storage must be in a dry nitrogen cabinet or desiccator to avoid native oxide growth and organic contamination.

  • Cleanroom Handling: Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers to avoid surface damage.
  • Storage Environment: Store sealed inside a dry nitrogen cabinet or cleanroom desiccator away from particulate dust and corrosive vapors.
  • Native Oxide Control: Bare prime silicon forms an ambient ~1–2 nm native SiO2 film in air, which must be removed before metallization or epitaxy if required.
  • Wet Processing Safety: All wet-chemical or cleanroom processing must strictly follow institutional EHS and SDS safety protocols.

Proper handling and cleaning procedures are essential to maintain wafer surface quality and ensure reproducible thin-film interfaces. Follow these steps to prepare wafers for processing.

Required Equipment: Cleanroom vacuum wand, PTFE/PEEK tweezers, Exhaust fume hood or wet bench

  1. Inspect wafer cassette
    Inspect the wafer cassette for any signs of damage or contamination before opening.
  2. Handle wafers by edge
    Handle wafers strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers.
  3. Degrease wafers
    Degrease diced dies or whole 2-inch wafers sequentially in acetone, electronic-grade isopropanol (IPA), and DI water.
  4. Dry wafers
    Blow-dry the wafers with nitrogen gas to remove residual solvents.
  5. Perform plasma descum
    Perform a mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.
  6. Remove native oxide if required
    Remove native oxide or perform RCA standard clean inside an exhaust fume hood or wet bench using facility-approved protocols.
  7. Store unused wafers
    Store unused wafers sealed inside the original 25-wafer polypropylene cassette box within a dry nitrogen cabinet.

What is the resistivity range of this 2-inch N-type <111> silicon wafer?

This wafer is Phosphorus-doped N-type with a verified resistivity of 0.01–0.1 Ω·cm, measured by four-point probe. This low-resistivity range (N+) provides low substrate contact resistance while maintaining lower free-carrier optical loss than degenerately doped N++ wafers, making it suitable for vertical diode fabrication, anodic glass bonding, and electrochemical electrodes.

Can this <111> silicon wafer be used for GaN or AlN epitaxial growth?

Yes. The <111> (± 0.5°) crystal orientation provides a hexagonal three-fold surface symmetry that supports lattice-matched III-nitride heteroepitaxy, including GaN, AlN, and SiC. The dual-side mirror-polished surface (DSP, Ra < 0.5 nm) and 275 ± 25 μm thickness are compatible with research-scale epitaxy chambers, and the bare prime silicon surface carries only a thin native oxide (~1–2 nm) for direct in-house epitaxial growth.

How should these 2-inch silicon wafers be stored and handled to maintain surface quality?

Store wafers sealed inside the original 25-wafer polypropylene cassette within a dry nitrogen cabinet or cleanroom desiccator to minimize airborne organic contamination and native oxide growth. Handle strictly by the perimeter edge using cleanroom vacuum wands or PTFE/PEEK tweezers, and avoid particulate dust and corrosive vapors. For processing, perform solvent pre-cleaning (acetone, IPA, DI water) followed by N2 blow-drying and mild O2 plasma descum prior to photoresist spin coating or PVD/ALD.

This 2-inch prime-grade CZ N-type <111> silicon wafer with 0.01–0.1 Ω·cm phosphorus doping and dual-side CMP finish (Ra < 0.5 nm) is engineered for hexagonal epitaxy, double-side lithography, and low-resistance device prototyping, but its bare surface, tight resistivity window, and cleanroom handling requirements impose strict environmental and procedural controls.

Positive

  • Low-Resistivity N+ Substrate: Phosphorus doping at 0.01–0.1 Ω·cm provides low substrate contact resistance while maintaining lower free-carrier optical loss than degenerately doped N++ wafers, supporting vertical diodes, anodic bonding, and electrochemical electrodes.
  • Dual-Side CMP Mirror Finish: Double-side polished surfaces with Ra < 0.5 nm enable double-sided MEMS patterning, through-wafer IR transmission, and direct fusion or anodic bonding without additional surface preparation.
  • <111> Lattice for Hexagonal Epitaxy: The densely packed <111> orientation with three-fold surface symmetry supports lattice-matched GaN, AlN, and SiC heteroepitaxy as well as UHV surface reconstruction studies.

Trade-offs

  • Bare Surface Requires Immediate Processing: Uncoated prime silicon forms a 1–2 nm native oxide in ambient air; users must perform solvent/plasma pre-cleaning or RCA wet processing before metallization or epitaxy to ensure reproducible interfaces.
  • Cleanroom Storage and Handling Mandate: Wafers must be stored in a dry nitrogen cabinet or desiccator and handled only by the perimeter edge with vacuum wands or PTFE/PEEK tweezers to prevent particulate and organic contamination.
  • Tight Resistivity Window Limits Flexibility: The specified 0.01–0.1 Ω·cm range constrains use to applications requiring this exact doping level; processes needing higher resistivity or degenerate doping will require a different substrate.

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

Pack Size

25 pcs

Diameter

2-Inch (50.8 ± 0.2 mm)

Growth Method

CZ (Czochralski)

Wafer Grade

Prime Grade (Virgin)

Conductivity & Dopant

N-Type / Phosphorus (P)

Orientation

± 0.5°

Resistivity

0.01-0.1 Ω·cm

Thickness

275 ± 25 μm

Surface Finish

Double-Side Polished (DSP, Ra < 0.5 nm)