FGH97 Spherical Nickel-Base Superalloy Powder

Price range: $474.00 through $538.00

Institutional Procurement & Supply Compliance: As a verified US supplier, Atomfair accepts formal institutional Purchase Orders (POs), contract billing schedules, and custom procurement loops for university and national laboratories, and corporate R&D departments globally.

Buy spherical superalloy FGH97 price deals for hot-end components turbine engines selective laser melting R&D. Aerospace industry standards. Contact inquiry@atomfair.com.

ATOMFAIR® FGH97

RESEARCH GRADE MATERIAL

Product Overview

Optimize structural consistency and mechanical reliability in high-temperature component validation using our premier spherical alloy framework. This powder system establishes superior layer-to-layer integrity during additive manufacturing, eliminating microstructural variance and serving as a stable high-performance baseline platform to meet targeted industrial pricing milestones.

Technical Specifications

PARAMETER DETAILS
1. Chemical Composition (wt.%)
Nickel (Ni) / Carbon (C) Balance / 0.02 – 0.06%
Chromium (Cr) / Cobalt (Co) 8.0 – 10.0% / 15.0 – 16.5%
Tungsten (W) / Molybdenum (Mo) 4.8 – 4.9% / 3.5 – 4.2%
Aluminum (Al) / Titanium (Ti) 4.85 – 5.25% / 1.6 – 2.0%
Iron (Fe) / Niobium (Nb) ≤0.5% / 2.4 – 2.8%
Tantalum (Ta) / Magnesium (Mg) 0.1 – 0.4% / 0.002 – 0.05%
Boron (B) / Zirconium (Zr) 0.006 – 0.015% / 0.01 – 0.015%
Cerium (Ce) / Silicon (Si) 0.005 – 0.01% / ≤0.20%
Manganese (Mn) ≤0.15%
2. Core Physical Design & Properties
Particle Size Range D10 ≥15 μm
Particle Size Range D50 30 – 40 μm
Particle Size Range D90 ≤60 μm
Sphericity ≥0.92
3. Typical Post-HIP & Heat-Treated Mechanical Parameters
Tensile Strength (750°C) ≥1250 MPa
Yield Strength (750°C) ≥900 MPa
Elongation (750°C) ≥15.0%
Manufacturing Rules Processed under strict aerospace industry standards conditions
Alternative Options Explore our related catalog or custom dimensions. For urgent technical custom requests or bulk inquiries, please contact our support team.

Key Features & Advantages

  • Homogeneous Material Purity: Features an uncompromised structural configuration with highly uniform elemental distribution across the matrix.
  • Enhanced Operational Efficiency: Specifically engineered to demonstrate superior electrochemical performance, significantly boosting transfer kinetics at targeted bands.
  • Optimized Sintering/Microstructure: Advanced synthesis allows for lower required operating temperatures and ideal grain boundary integration during cell fabrication.

APPLICATION SCOPE: Highly optimized for hot-end components of turbine engines, encompassing turbine discs, shafts, and annular parts which serve as critical structural elements.
PACKAGING: Sealed argon-filled protective bottles or specialized vacuum containment drums.
IMPORTANT NOTICE: This product is highly sensitive to ambient exposure. Keep containers tightly sealed or handle exclusively within an anhydrous inert gas environment to prevent phase contamination or degradation before thermal validation.
TAILORED SOLUTIONS FOR RESEARCH
Contact our engineering team for technical support or official institutional quotations.
EMAIL: inquiry@atomfair.com
Manufacturer: Atomfair LLC
Brand: ATOMFAIR®

Every advanced material, component, equipment, and instrument in our catalog is backed by rigorous testing. We maintain strict internal quality management frameworks and align with CE conformity metrics to deliver transparent, reproducible performance data via our public open-science repository.

To request raw batch performance data, submit formal vendor registration paperwork, or execute a fast-turnaround R&D manufacturing loop, contact us at inquiry@atomfair.com.

Item is dispatched under the Atomfair Shipping & Delivery Framework (Free worldwide shipping on orders over $59 USD excl. heavy equipment). Return is governed by the Atomfair Return & Refund Policy (7-day technical return window).

size

1kg0-15μm, 1kg0-25μm, 1kg15-45μm