| PARAMETER |
DETAILS |
| 1. Core Device & Electrochemical Design |
| Product Structural Configuration |
Bimodal (7:3 ratio blend of big spherical & small single crystal) |
| Specific Surface Area (SSA BET) |
0.56 m²/g |
| Tap Density (TD) |
2.46 g/cm³ |
| Pellet Density (PD) |
3.63 g/cm³ |
| Surface Residual Alkali Li₂CO₃ |
0.25 % |
| Surface Residual Alkali LiOH |
0.30 % |
| pH Value |
11.6 |
| 2. Cathode (Positive Electrode) Parameters |
| 0.1C Charge Specific Capacity |
244.2 mAh/g (Coin Cell Half-Cell, 3.0V–4.3V) |
| 0.1C Discharge Specific Capacity |
220.8 mAh/g (Coin Cell Half-Cell, 3.0V–4.3V) |
| Initial Coulombic Efficiency (ICE) |
90.4 % |
| 0.5C Discharge Rate Capacity |
206.6 mAh/g |
| 1.0C Discharge Rate Capacity |
200.7 mAh/g |
| Target Cathode Electrode Density |
3.5 g/cm³ |
| 3. Anode (Negative Electrode) Parameters |
| Testing Counter Electrode Configuration |
Lithium Metal Target Half-Cell Foils |
| 4. Separator & Physical Package Metrics |
| Particle Size Distribution Dmin / Dmax |
1.2 μm / 25.4 μm |
| Particle Size Distribution D10 |
2.3 μm |
| Particle Size Distribution D50 |
10.1 μm |
| Particle Size Distribution D90 |
18.3 μm |
| Transition Metal Molar Ratio (ICP) |
Ni: 91.1 mol% | Co: 5.5 mol% | Mn: 3.4 mol% |
| Core Base Element Content |
Li: 7.4 % |
| Chemical Impurity Profile (ICP) |
Fe: 0 ppm | Na: 40 ppm | Ca: 12 ppm | Cu: 0 ppm | S: 500 ppm |
| Manufacturing Rules |
Processed under strict RoHS compliant standard conditions |
| Alternative Options |
Explore our related catalog or custom dimensions. For urgent technical custom requests or bulk inquiries, please contact our support team. |