| PARAMETER |
DETAILS |
| 1. Core Device & Electrochemical Design |
| Product Structural Configuration |
Medium Nickel Mono Crystal Type |
| Specific Surface Area (BET) |
0.804 m²/g |
| Tap Density (TD) |
2.08 g/cm³ |
| Pellet Density (PD powder) |
3.02 g/cm³ |
| Surface Residual Alkali LiOH |
0.0764 %wt |
| Surface Residual Alkali Li₂CO₃ |
0.1103 %wt |
| pH Value |
10.62 |
| 2. Cathode (Positive Electrode) Parameters |
| 0.1C Charge Specific Capacity |
219.3 mAh/g (CR2032 Coin Cell, 3.0V–4.4V) |
| 0.1C Discharge Specific Capacity |
198.0 mAh/g (CR2032 Coin Cell, 3.0V–4.4V) |
| Initial Coulombic Efficiency (Eff) |
90.28 % |
| 0.5C Discharge Capacity |
188.9 mAh/g |
| 1.0C Discharge Capacity |
184.1 mAh/g |
| 2.0C Discharge Capacity |
180.2 mAh/g |
| Initial DCR (10% SOC @ 25°C) |
13.98 Ω |
| Initial DCR (50% SOC @ 25°C) |
38.26 Ω |
| Thermal DSC Peak Temp (4.40V) |
233.4 °C (without electrolyte) |
| 3. Anode (Negative Electrode) Parameters |
| Testing Counter Electrode Configuration |
Lithium Metal Target Half-Cell Foils / Pouch-cell vs. Graphite |
| 4. Separator & Physical Package Metrics |
| Particle Size Distribution D0 / D100 |
1.282 μm / 7.634 μm |
| Particle Size Distribution D10 |
2.226 μm |
| Particle Size Distribution D50 |
3.524 μm |
| Particle Size Distribution D90 |
5.424 μm |
| Main Weight Component Profiles |
Ni: 38.72 %wt | Co: 8.79 %wt | Mn: 11.00 %wt | Li: 7.30 %wt |
| Transition Metal Molar Ratio (mol%) |
Ni: 65.38 mol% | Co: 14.78 mol% | Mn: 19.84 mol% |
| Trace Chemical Impurities profile |
S: 588 %wt |
| Manufacturing Rules |
Processed under strict RoHS compliant standard conditions |