| PARAMETER |
DETAILS |
| 1. Core Device & Electrochemical Design |
| Product Structural Configuration |
Medium Nickel Mono Crystal Type |
| Specific Surface Area (BET) |
0.871 m²/g |
| Tap Density (TD) |
2.01 g/cm³ |
| Pellet Density (PD powder) |
3.04 g/cm³ |
| Surface Residual Alkali LiOH |
0.0636 %wt |
| Surface Residual Alkali Li₂CO₃ |
0.0729 %wt |
| pH Value |
11.21 |
| 2. Cathode (Positive Electrode) Parameters |
| 0.1C Charge Specific Capacity |
217.6 mAh/g (CR2032 Coin Cell, 3.0V–4.4V) |
| 0.1C Discharge Specific Capacity |
195.2 mAh/g (CR2032 Coin Cell, 3.0V–4.4V) |
| Initial Coulombic Efficiency (Eff) |
89.7 % |
| 0.5C Discharge Capacity |
184.1 mAh/g |
| 1.0C Discharge Capacity |
177.6 mAh/g |
| 2.0C Discharge Capacity |
171.0 mAh/g |
| Initial DCR (10% SOC @ 25°C) |
14.37 Ω |
| Initial DCR (50% SOC @ 25°C) |
40.63 Ω |
| Thermal DSC Peak Temp (4.40V) |
245.2 °C (without electrolyte) |
| 3. Anode (Negative Electrode) Parameters |
| Testing Counter Electrode Configuration |
Lithium Metal Target Half-Cell Foils / Pouch-cell vs. Graphite |
| 4. Separator & Physical Package Metrics |
| Particle Size Distribution D0 / D100 |
0.408 μm / 9.244 μm |
| Particle Size Distribution D10 |
1.921 μm |
| Particle Size Distribution D50 |
3.810 μm |
| Particle Size Distribution D90 |
6.721 μm |
| Main Weight Component Profiles |
Ni: 36.02 %wt | Co: 6.01 %wt | Mn: 16.65 %wt | Li: 7.24 %wt |
| Transition Metal Molar Ratio (mol%) |
Ni: 60.24 mol% | Co: 10.01 mol% | Mn: 29.75 mol% |
| Trace Chemical Impurities profile |
S: 735 %wt |
| Manufacturing Rules |
Processed under strict RoHS compliant standard conditions |
| Alternative Options |
Explore our related catalog or custom dimensions. For urgent technical custom requests or bulk inquiries, please contact our support team. |