Atomfair GH3536 Nickel-Based Superalloy Powder

GH3536 is a Ni-based solid solution-strengthened superalloy, featuring excellent oxidation and corrosion resistance, good hot/cold work formability, and weldability. It offers moderate creep and rupture strength below 900°C, ideal for long-service aero-engine parts like combustion chamber components, honeycomb structures, diffusers, and other hot-end parts. Compatible with SLM.

Description

Chemical Composition (wt.%)
C 0.05-0.15
Cr 20.5-23.0
Ni Balance
Co 0.5-2.5
W 0.2-1.0
Fe 8.0-10.0
Ni ≤0.5
Ti ≤0.15
Fe 17.0-20.0
B ≤0.01
Si ≤1.0
Mn ≤1.0
P ≤0.025
S ≤0.015
Cu ≤0.5
O ≤0.02
N ≤0.02
Physical Properties
Particle Size (μm) D10≥15, D50 30-40, D90≤58
Sphericity ≥0.9
Apparent Density (g/cm³) ≥4.4
Tapped Density (g/cm³) ≥5.0
Flowability (s/50g) ≤18
Mechanical Properties (Solution Treated)
Room Temp 900°C
Tensile: ≥700MPa
Yield: ≥300MPa
Elongation: ≥20.0%
Tensile: ≥220MPa
Yield: ≥170MPa
Elongation: ≥20.0%