NEPEM N-417 Composite Ion Exchange Membrane for Electrolysis/Electroplating

The NEPEM Composite PEM is fabricated via a proprietary tape casting process using perfluorosulfonic acid resin with optimized molecular weight and ion exchange capacity. It features uniform thickness and is widely applied in electrolytic industries such as electrolytic chlorine dioxide generators, etching solution copper recovery, gold salt preparation, amino acid refining, caustic soda production, and electrodialysis.

Description

Uniform thickness membrane for chlorine dioxide generators, metal recovery, and electrodialysis applications.

Thickness and Basis Weight
Thickness (ฮผm) 260
Weight (g/mยฒ) 340
Physical Properties (23ยฐC,50%RH)
Tensile Strength (MPa) โ‰ฅ40
Elongation at Break (%) โ‰ฅ100
Specific Gravity 1.35
Performance
Conductivity (S/cm, 23ยฐC,100%RH) โ‰ฅ0.100
Acid Capacity (meq/g) 1.00ยฑ0.05
Hydrolytic Properties
Water Content (%) 5.0ยฑ3.0
Water Uptake (%) 50.0ยฑ5.0
Thickness Change (23ยฐC water, %) โ‰ค5
Thickness Change (100ยฐC water, %) โ‰ค10
Linear Expansion (23ยฐC water, %) โ‰ค2
Linear Expansion (100ยฐC water, %) โ‰ค5